碳化钨薄膜在100 keV Kr+离子辐照下的侵蚀研究
Erosion Study of Tungsten Carbide films under 100 keV Kr+ ion irradiation
AI总结:
本研究利用RF溅射在400 K和600 K下制备WC薄膜,经100 keV Kr+离子辐照后,通过GIXRD和RBS分析发现两种薄膜的侵蚀速率均约为每个入射离子1.6个原子,为极端辐射环境下WC薄膜的耐辐射性能提供了基础理解。
摘要:
碳化钨(WC)因其抗辐射性和优异的机械强度,成为极端环境探索的关键材料。WC广泛应用于切削工具、高磨损部件,并作为核反应堆中等离子体面对材料的潜在候选者,其在替代辐照下的侵蚀行为是研究的课题。在本工作中,使用RF溅射在400 K和600 K两种不同基底温度下合成了WC薄膜,随后在1x10^17 ions/cm2的注量下用100 keV Kr1+离子进行辐照。通过掠入射X射线衍射(GIXRD)测量确认了沉积态WC薄膜的晶相。采用卢瑟福背散射谱法(RBS),通过测量原始和辐照薄膜面密度的差异,确定了原始样品的厚度和溅射速率。发现两种薄膜的侵蚀速率均为每个入射Kr+离子约1.6个原子。这些发现有助于对WC薄膜辐射耐受行为的基础理解,这对于其在极端辐射的苛刻条件下的性能至关重要。
英文摘要:
Tungsten carbide (WC) stands out as a crucial material for exploration in extreme environments due to its resistance to radiation and impressive mechanical strength. Widely utilized in cutting tools, high-wear components, and as a potential contender for plasma-facing material in nuclear reactors, WC's erosion behavior under surrogate irradiations is a subject of investigation. In the present work, WC films were synthesized at two different substrate temperatures of 400 K and 600 K using RF sputtering and were then irradiated with 100 keV Kr1+ ions at a fluence of 1x1017 ions/cm2. The crystalline phases of as deposited WC films were confirmed by glancing incidence X-ray diffraction (GIXRD) measurements. Rutherford Backscattering Spectrometry (RBS) was employed to determine the thicknesses of pristine samples and the sputtering rate by measuring the difference in the areal densities of the pristine and irradiated films. The erosion rate of both types of films was found to be ~ 1.6 atoms per incident Kr+ ion. These findings contribute to a foundational comprehension of the radiation tolerance behavior of WC thin films, crucial for their performance in the demanding conditions of extreme radiation.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。