arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2401.00646cond-mat.str-elcond-mat.mtrl-sci
收藏

(Ni0.93Co0.07)3V2O8的高磁场相图与弱铁磁破缺

High magnetic field phase diagram and weak FM breaking in (Ni0.93Co0.07)3V2O8

Jiating Wu, Minjie Zhang, Ke Shi, Huxin Yin, Yuyan Han, Lansheng Ling, Wei Tong, Chuanying Xi, Li Pi, Zhaosheng Wang

AI总结:

通过磁致伸缩和热膨胀测量构建了(Ni0.93Co0.07)3V2O8沿a、b、c方向高达33 T的高磁场相图,发现多个中间相和混合态,并揭示Co2+掺杂破坏了公度相的弱铁磁矩,影响自旋调制。

摘要:

我们报道了多铁性材料(Ni0.93Co0.07)3V2O8的磁致伸缩和热膨胀测量结果。构建了沿a、b、c方向高达33 T的高磁场相图。对于H//a,随着磁场增加,在约7 K时,非公度相与顺磁相之间出现两个中间相,随后在顺磁相之上出现一个磁致诱导相。对于H//b,热膨胀测量表明高磁场相的自旋-晶格耦合发生突变。交错的相边界暗示光学高磁场相中存在混合态。对于H//c,检测到公度相与非公度相之间的一个中间相。发现中间相与低温非公度相之间存在非线性边界,以及公度相与顺磁相之间存在清晰边界。这些结果表明,掺杂Co2+破坏了公度相的弱铁磁矩,该弱铁磁矩存在于母体化合物Ni3V2O8和(Ni0.9Co0.1)3V2O8中。这种非线性影响反映了通过掺杂Co2+对Ni3V2O8中复杂自旋调制的调控。

英文摘要:

We present magnetostriction and thermal expansion measurements on multiferroic (Ni0.93Co0.07)3V2O8. The high field phase diagrams up to 33 T along the a, b and c directions are built. For H//a, as the magnetic field increases, two intermediate phases appear between the incommensurate phase and the paramagnetic phase at about 7 K, and then a magnetically induced phase appears above the paramagnetic phase. For H//b,thermal expansion measurement indicates a mutation in the spin lattice coupling of the high field phases. The interlaced phase boundary suggests a mixed state in the optical high field phase. For H//c, an intermediate phase between the commensurate phase and the incommensurate phase is detected. A nonlinear boundary between the intermediate phase and the low temperature incommensurate phase, and a clear boundary between the commensurate phase and the paramagnetic phase are found. These results indicate that doping Co2+ breaks the weak ferromagnetic moment of the commensurate phase, which exists in the parent compound Ni3V2O8 and (Ni0.9Co0.1)3V2O8. This nonlinear influence reflects complicated spin modulation in Ni3V2O8 by doping Co2+.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑