Pulsed laser deposition has been used to deposit Y1Ba2Cu3O7 layer on CeO2 buffer layers on (1102) sapphire. Both layers are epitaxial with the (110) direction of the CeO2 layer aligned with the <2021> direction of the sapphire substrate. The c-axis Y1Ba2Cu3O7 layer has its <100> direction aligned with the <110> direction of the CeO2. Cross-sectional transmission electron microscopy shows the epitaxy to be coherent and the interfaces to be abrupt at an atomic level. The best films have a critical current of 9 e6 A/cm2 at 4.2 K and lower microwave surface resistance than copper at 77 K and at a frequency of 31 GHz.
Properties of YBa$_2$Cu$_3$O$_{7-δ}$ films grown by pulsed laser deposition on CeO$_2$-buffered sapphire
本文研究了用脉冲激光沉积法在r切蓝宝石衬底上生长$_2$ $_3$ O $_{7-δ}$(YBCO)薄膜。为了改善衬底和薄膜之间的晶格参数的匹配,我们使用CeO $_{2}$缓冲层,再结晶之前的YBCO的沉积。首先使用原子力显微镜(AFM)和X射线衍射确定缓冲层的最佳再结晶厚度和温度。接下来,我们使用原子力显微镜来检查薄膜厚度上的YBCO薄膜的粗糙度的依赖性,我们研究的均匀性的磁通渗透到薄膜的磁光成像。我们发现这些薄膜的超导临界温度和临界电流密度与生长在匹配衬底上的YBCO薄膜非常相似。看来,YBCO薄膜的微结构的影响,在缓冲层中的结构缺陷,以及在氧不足的变化,这导致在高的临界电流密度值适用于应用。
K-doped Ba122 epitaxial thin film on MgO substrate by buffer engineering
在MgO衬底上实现了K掺杂Ba 122(Ba $_{1-x}$ K $_x$ Fe $_\text{2}$ As $_\text{2}$)超导体的分子束外延。显微结构观察表明,未掺杂的Ba 122作为一个完美的缓冲层的K掺杂Ba 122的外延生长。该薄膜在4K时具有39.8 K的高临界温度和3.9 MA/cm $^\text{2}$的高临界电流密度。外延薄膜的成功生长将使在氧化物双晶衬底上实现人工单晶界成为可能,并揭示了K掺杂Ba 122的晶界输运性质。
Freestanding GdBa2Cu3O7 Thin Films via Optimized Buffer Layer Design: Preserving Superconducting Properties
College of Industrial Technology, Nihon University(日本大学产业技术学部);Institute for Technical Physics, Karlsruhe Institute of Technology(卡尔斯鲁厄理工学院技术物理研究所);Department of Materials Physics, Nagoya University(名古屋大学物质物理学系);The Ultramicroscopy Research Center, Kyushu University(九州大学超显微研究中心);Department of Advanced Materials Science and Engineering, Kyushu University(九州大学先进材料科学与工程系);Interdisciplinary Graduate School of Engineering Sciences, Kyushu University(九州大学工学研究科交叉研究生院)