Previous studies have shown that type-II magnetic domain contrasts are caused by differences in the backscattering yields of magnetic domains of opposite magnetisation. Imaging the magnetic domains when the magnetisation vectors in the opposite-magnetisation domains are perpendicular to the tilt axis of the specimen has been considered impossible, because of the lack of change in the backscattering yields between the domains. However, we found that it is possible to observe the type-II magnetic domain contrast even in cases where the backscattering coefficients of the domains are the same. The contrast arises from the electron-scattering anisotropy created because of the deflection of the electron trajectories by the Lorentz force. We verify this by distinguishing all four possible in-plane magnetisation vectors on a Fe-Si(100) surface, using an electron backscatter diffraction detector as an arrya of electron detectors. The change in contrast between the magnetic domains, with respect to the location of a virtual electron detector, can provide information on the directions of the magnetisation vectors. A method to suppress the topographic contrast superimposed on the magnetic domain contrast is also demonstrated.
Direct measurement of the magnetic anisotropy field in Mn--Ga and Mn--Co--Ga Heusler films
研究了四方形变Mn-Ga基合金的静态和动态磁性能。在高达6.5 T的磁场中使用SQUID磁强计测定静态性质。纯Mn $_{1.6}$ Ga薄膜的饱和磁化强度为0.36 MA/m,矫顽力为0.29 T. Mn被Co部分取代产生Mn $_{2.6}$ Co $_{0.3}$ Ga $_{1.1}$。这些薄膜的饱和磁化强度下降到0.2~MA/m,矫顽力提高到1~T。利用时间分辨磁光克尔效应(TR-MOKE)研究了Mn-Ga的高频动力学行为。外推到零场的铁磁共振频率为125~GHz,吉尔伯特阻尼$α$为0.019。由SQUID和TR-MOKE确定的各向异性场为4.5 T,对应于0.81 MJ/m $^3$的有效各向异性密度。给定Mn $_{2.6}$ Co $_{0.3}$ Ga $_{1.1}$膜的大的各向异性场,使用高达60 T的脉冲磁场来确定使膜在平面中饱和所需的场强。为此,采用了非常的霍尔效应作为局部磁化强度的探针。通过对重构的面内磁化曲线进行积分,确定Mn $_{2.6}$ Co $_{0.3}$ Ga $_{1.1}$的有效各向异性能量密度为1.23 MJ/m $^3$ .
Finite-size versus Surface effects in nanoparticles
我们研究了有限尺寸和表面效应对小磁性粒子磁化强度的热行为和空间行为的影响。我们考虑两个系统:1)具有周期边界条件或自由边界条件的简单立方结构的盒形各向同性粒子。这种情况下,分析处理使用的各向同性模型的D-分量自旋矢量的限制$D\to \infty$,包括磁场。2)更真实的颗粒($γ$-Fe $_{2}$ O $_{3}$),具有开放边界的椭圆形(或球形)形状。该粒子的磁状态由各向异性的经典Dirac-Heisenberg模型描述,包括交换和偶极相互作用,以及体积和表面各向异性。这种情况下处理的经典蒙特卡罗技术。结果表明,在这两个系统中的有限尺寸效应产生的磁化强度的积极贡献,而表面效应呈现较大的和负的贡献,导致相对于散装系统的小颗粒的磁化强度的净减少。在系统2)中,两个贡献之间的差异通过表面各向异性而增强。后者还导致在低温下磁化强度的不饱和,表明颗粒核心中的磁序被表面上的磁无序扰动。这是由磁化曲线证实的。
A spin dynamics study in layered van der Waals single crystal, Cr$_2$Ge$_2$Te$_6$
利用宽带铁磁共振(FMR)技术研究了Cr $_2$ Ge $_2$ Te $_6$(CGT)大块单晶在60 K至2 K温度范围内的磁化动力学.我们确定的基FMR模式作为频率和静态磁场的磁晶易轴和难轴的函数的Kittel关系。提取的单轴磁晶各向异性常数和饱和磁化强度相比,当归一化与它们的低温值。当以对数标度绘制时,比值显示出明显的温度依赖性,这与预测的Callen-Callen幂律拟合直线不同,其中标度指数\textit{n},$K_{u}(T) \propto [M_s(T)/M_s(2$ K $)]^n$与单轴各向异性的预期值3相矛盾。此外,磁易轴和磁难轴的光谱g因子都表现出温度依赖性,反演在20 K和30 K之间,表明受到轨道角动量的影响。最后,我们定性地讨论了在低于饱和磁化强度的磁场下,在FMR谱中观察到的多畴共振现象。
Coercivity weighted Langevin magnetisation; A new approach to interpret superparamagnetic and nonsuperparamagnetic behaviour in single domain magnetic nanoparticles
Magnetic properties of exchange biased and of unbiased oxide/permalloy thin layers: a ferromagnetic resonance and Brillouin scattering study
微带铁磁共振和布里渊散射是用来提供一个比较确定薄坡莫合金层的磁性参数与非磁性(Al 2 O 3)或与反铁磁氧化物(NiO)。结果表明,垂直各向异性监测的界面表面能项,这是实际上独立的界面的性质。在厚度(5-25 nm)的调查间隔的饱和磁化强度没有显着不同,从报告的散装坡莫合金。面内单轴各向异性和交换偏置各向异性也来自于动态磁激发的研究,并与我们使用常规磁力测量的独立评估进行了比较
An integrated approach to doped thin films with strain tunable magnetic anisotropy: Powder synthesis, target preparation and pulsed laser deposition of Bi:YIG
Ab initio calculated diamagnetic and paramagnetic susceptibility of carbonate minerals
Institute of Geophysics of the Czech Academy of Sciences(捷克科学院地球物理研究所);Faculty of Nuclear Sciences and Physical Engineering, Czech Technical University(捷克理工大学核科学与物理工程学院);Faculty of Mathematics and Physics, Charles University(查理大学数学与物理学院)
Integrated ab initio modelling of atomic order and magnetic anisotropy for rare-earth-free magnet design: effects of alloying additions in $\mathrm{L}1_0$ FeNi
Stress-tailoring magnetic anisotropy of V$_2$O$_3$/Ni bilayers
本文报道了V $_2$ O $_3$ /Ni双层膜在温度驱动下的面内磁各向异性的可逆变化。这是由于在$T_C$ = 160 K时V $_2$ O $_3$的菱面体到单斜结构相变引起的。平面内磁各向异性在$T_C$以上是单轴的,但是当双层通过结构相变冷却时,出现第二磁易轴。铁磁共振测量表明,这种磁各向异性的变化是可逆的温度。我们确定了两个结构特性的V $_2$ O $_3$ /Ni双层膜影响面内磁各向异性:(1)生长诱导的单轴磁各向异性与双层微结构中的阶梯状台阶和(2)低温应变诱导的双轴各向异性与V $_2$ O $_3$结构相变。磁电阻测量证实了磁各向异性的变化在整个结构转变,并建议镍的负磁致伸缩导致应变诱导的易轴的出现。这表明V $_2$ O $_3$中的温度依赖性结构转变可用于调节相邻铁磁薄膜中的磁各向异性。