arXiv 2302.08654cond-mat.mtrl-sci
收藏

放电等离子烧结合成高硬度ReB2-type中熵二硼化物(W1/3Re1/3Ru1/3)B2

Spark plasma sintering synthesis of ReB2-type medium-entropy diboride (W1/3Re1/3Ru1/3)B2 with high hardness

Wuzhang Yang, Guorui Xiao, Zhi Ren

摘要:

采用放电等离子烧结法在1600 ℃下合成了一种新的中熵二硼化物(MEDB)(W_(1/3)Re_(1/3)Ru_(1/3))B_2。尽管WB 2、ReB 2和RuB 2的结构不同,但烧结的MEDB由单一六方ReB 2型相(空间群P63/mmc)组成,相对密度为94.2%,平均晶粒尺寸为6.8 $\pm$ 2.2 μ m。结构细化和电子显微镜测量表明,W,Re和Ru原子占据相同的晶体学位置,并均匀分布在晶格中。(W1/3Re 1/3Ru 1/3)B2 MEDB在0.49 N的载荷下具有30.7 GPa的维氏硬度,在9.8 N的载荷下具有20.5 GPa的维氏硬度,这与针对单个二元对应物所报道的维氏硬度相当或更高。

英文摘要:

A new medium-entropy diboride (MEDB) (W1/3Re1/3Ru1/3)B2 has been synthesized by spark plasma sintering of elemental powders at 1600 oC. Despite the dissimilar structures of WB2, ReB2 and RuB2, the sintered MEDB consists of a single hexagonal ReB2-type phase (space group P63/mmc) with a relative density of 94.2% and an average grain size of 6.8 $\pm$ 2.2 um. Structural refinement and electron microscopy measurements show that the W, Re, and Ru atoms occupy the same crystallographic site and are distributed uniformly in the lattice. The (W1/3Re1/3Ru1/3)B2 MEDB has Vickers hardnesses of 30.7 GPa at a load of 0.49 N and 20.5 GPa at a load of 9.8 N, which are comparable or higher than those reported for individual binary counterparts.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑