从晶格畸变揭示高熵陶瓷的硬化与强化机制
Unrevealing hardening and strengthening mechanisms in high-entropy ceramics from lattice distortion
AI总结:
本研究以高熵二硼化物为原型,通过实验与第一性原理计算,揭示晶格畸变加剧伴随B-B键强化是高熵陶瓷硬度和抗弯强度提升的核心机制,为超硬高强度高熵陶瓷设计提供指导。
摘要:
揭示硬化与强化机制对于推动超硬、高强度高熵陶瓷(HECs)的设计至关重要。本文以高熵二硼化物(HEB₂)为原型,系统研究高熵陶瓷的硬化与强化机制。具体而言,采用超快速高温烧结法制备了等原子比的4至9种阳离子单相HEB₂陶瓷(4-9HEB₂)。所制备的4-9HEB₂样品具有相近的晶粒尺寸、相当的相对密度(最高约98%)、均匀的成分以及无杂质的洁净晶界。实验结果表明,4-9HEB₂样品的硬度和抗弯强度随金属组元数量的增加呈上升趋势。第一性原理计算发现,晶格畸变对HEB₂的硬度和强度起关键作用。随着金属组元数量增加,晶格畸变加剧,同时B-B键得到强化,从而提升了硬度和抗弯强度。此外,研究还否定了其他潜在指标与HEB₂硬度/抗弯强度的相关性,包括价电子浓度、电负性失配和金属态。本研究揭示了通过加剧晶格畸变实现高熵陶瓷硬化与强化的机制,可为开发超硬、高强度高熵陶瓷提供指导。
英文摘要:
Revealing the hardening and strengthening mechanisms is crucial for facilitating the design of superhard and high-strength high-entropy ceramics (HECs). Here, we take high-entropy diborides (HEB$_2$) as the prototype to thoroughly investigate the hardening and strengthening mechanisms of HECs. Specifically, the equiatomic 4- to 9-cation single-phase HEB$_2$ ceramics (4-9HEB$_2$) are fabricated by an ultra-fast high-temperature sintering method. The as-fabricated 4-9HEB$_2$ samples possess similar grain sizes, comparable relative densities (up to ~98%), uniform compositions, and clean grain boundaries without any impurities. The experimental results show that the hardness and flexural strength of the as-fabricated 4-9HEB$_2$ samples have an increasing tendency with the increase of metal components. The first-principles calculations find that lattice distortion is essential to the hardness and strength of HEB$_2$. With the increase of metal components, an aggravation of lattice distortion accompanied by B-B bond strengthening is determined, resulting in the enhancement of the hardness and flexural strength. Moreover, the correlation between other potential indicators and the hardness/flexural strength of HEB$_2$ has been disproved, including valence electron concentration, electronegativity mismatch, and metallic states. Our results unravel the hardening and strengthening mechanisms of HECs by intensifying lattice distortion, which may provide guidance for developing superhard and high-strength HECs.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。