Laser-Induced Cavitation for Controlling Crystallization from Solution
AI总结:
本文利用低于击穿阈值的Nd:YAG激光脉冲产生空化泡,在过饱和水溶液中诱导结晶,并通过高速视频显微镜与模拟揭示激光能量耗散竞争如何决定界面过饱和度峰值,从而调控晶体数量与形貌。
摘要:
我们证明,由低于击穿阈值的Nd:YAG激光脉冲引发的空化泡能够从过饱和水溶液中诱导结晶,且成核动力学依赖于过饱和度和激光能量。结合高速视频显微镜与模拟,我们认为吸收的激光能量以潜热和显热形式耗散之间的竞争决定了溶剂蒸发速率,并在气液界面处产生瞬时的过饱和度峰值。晶体的数量和形貌与模拟得到的过饱和度峰值特征相关。
英文摘要:
We demonstrate that a cavitation bubble initiated by a Nd:YAG laser pulse below breakdown threshold induces crystallization from supersaturated aqueous solutions with supersaturation and laser-energy dependent nucleation kinetics. Combining high-speed video microscopy and simulations, we argue that a competition between the dissipation of absorbed laser energy as latent and sensible heat dictates the solvent evaporation rate and creates a momentary supersaturation peak at the vapor-liquid interface. The number and morphology of crystals correlate to the characteristics of the simulated supersaturation peak.