arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2111.12191cond-mat.mtrl-sci
收藏

利用极化中子反射测量技术探究软磁-硬磁双层膜中的磁构型调控

Controlling magnetic configuration in soft-hard bilayers probed by polarized neutron reflectometry

Nan Tang, Jung-Wei Liao, Siu-Tat Chui, Timothy Ziman, Kai Liu6 Chih-Huang Lai, Brian J. Kirby, Dustin A. Gilbert

AI总结:

本文利用极化中子反射测量技术系统研究了软磁/硬磁双层膜的界面磁构型,发现其高度依赖于软磁层厚度和饱和磁化强度,而受硬磁层参数影响较弱,为复合磁体的性能调控提供了设计依据。

摘要:

硬磁/软磁双层薄膜已广泛应用于数据存储技术和永磁体应用中。这些异质结构中的磁构型及其对温度和磁场的响应被认为高度依赖于界面耦合。然而,各层自身的本征性质,如饱和磁化强度和层厚,也会强烈影响磁构型。改变这些参数为调控复合磁体的磁性能提供了一种有效方法。在此,我们利用极化中子反射测量技术(PNR)实验探测了硬磁/软磁双层薄膜中的界面磁构型,所研究的体系包括:L10-FePt/A1-FePt、[Co/Pd]/CoPd、[Co/Pt]/FeNi 和 L10-FePt/Fe,这些薄膜的硬磁层均具有垂直磁各向异性。这些薄膜分别设计了不同的软磁层和硬磁层厚度(t_soft 和 t_hard)以及饱和磁化强度(M_s^soft 和 M_s^hard)。此外,利用 L10-FePt/A1-FePt 双层样品研究了面内磁场(H_ip)和温度(T)的影响。将 PNR 结果与微磁学模拟对比表明,界面磁构型高度依赖于 t_soft、M_s^soft 以及外部因素(H_ip 和 T),而对 t_hard 和 M_s^hard 的依赖性相对较弱。这些结果中关键的一点是:对于较薄的 t_soft,硬磁层和软磁层在面外方向刚性耦合,随后发生向面内弛豫的转变。通过降低 M_s^soft,可以将这一转变推迟到更大的 t_soft。理解这些参数对磁构型的影响对于设计面向应用的 functional 复合磁体至关重要。

英文摘要:

Hard/soft magnetic bilayer thin films have been widely used in data storage technologies and permanent magnet applications. The magnetic configuration and response to temperatures and magnetic fields in these heterostructures are considered to be highly dependent on the interfacial coupling. However, the intrinsic properties of each of the layers, such as the saturation magnetization and layer thickness, also strongly influence the magnetic configuration. Changing these parameters provides an effective method to tailor magnetic properties in composite magnets. Here, we use polarized neutron reflectometry (PNR) to experimentally probe the interfacial magnetic configurations in hard/soft bilayer thin films: L10-FePt/A1-FePt, [Co/Pd] /CoPd, [Co/Pt] /FeNi and L10-FePt/Fe, which all have a perpendicular magnetic anisotropy in the hard layer. These films were designed with different soft and hard layer thicknesses (t_soft and t_hard) and saturation magnetization (M_s^soft and M_s^hard), respectively. The influences of an in-plane magnetic field (H_ip) and temperature (T) are also studied using a L10 FePt/A1-FePt bilayer sample. Comparing the PNR results to micromagnetic simulations reveals that the interfacial magnetic configuration is highly dependent on t_soft, M_s^soft and the external factors (H_ip and T), and has a relatively weak dependence on t_hard and M_s^hard. Key among these results, for thin t_soft, the hard and soft layers are rigidly coupled in the out-of-plane direction, then undergo a transition to relax in-plane. This transition can be delayed to larger t_soft by decreasing M_s^soft. Understanding the influence of these parameters on the magnetic configuration is critical to designing functional composite magnets for applications.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑