Medium-Mn steels exhibit excellent mechanical properties and lower production costs compared to high-Mn steels, which makes them a potential material for future application in the automotive industry. Intercritical annealing (ICA) after cold rolling allows to control the stacking fault energy (SFE) of austenite, the fraction of ferrite and reverted austenite, and the element partitioning (especially Mn). Although Mn deteriorates the corrosion behavior of Fe-Mn-Al alloys, the influence of austenite fraction and element partitioning of Mn on the electrochemical corrosion behavior has not been investigated yet. Therefore, the electrochemical corrosion behavior in 0.1 M H2SO4 of X6MnAl12-3, which was intercritically annealed for 2 h at 550 °C, 600 °C and 700 °C, was investigated by potentiodynamic polarization (PDP), electrochemical impedance spectroscopy (EIS) and mass spectroscopy with inductively coupled plasma (ICP-MS). Additionally, specimens after 1 h and 24 h of immersion were examined via SEM to visualize the corrosion damage. The ICA specimens showed a selective dissolution of reverted austenite due to its micro-galvanic coupling with the adjacent ferrite. The severity of the micro-galvanic coupling can be reduced by decreasing the interface area as well as the chemical gradient of mainly Mn between ferrite and reverted austenite by ICA.
Effect of ECAP and heat treatment on mechanical properties, stress relaxation behavior and corrosion resistance of a 321-type austenitic steel with increased delta-ferrite content
Corrosion Evolution of T91 Steel in Static Lead-Bismuth Eutectic Under an Oxidising Environment
University of Oxford(牛津大学);Max-Planck-Institute for Sustainable Materials(马克斯·普朗克可持续材料研究所);Massachusetts Institute of Technology(麻省理工学院);Australia's Nuclear Science and Technology Organisation(澳大利亚核科学与技术组织)
Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500$^\circ$C
研究了316 L和DIN 1.4970奥氏体不锈钢与贫氧(C $_O$ < 10 $^-$ $^8$质量%)静态液态铅铋共晶(LBE)在500°C下接触600-1000 h后的溶解腐蚀行为的早期阶段($\le$ 1000 h)。本研究的目的是确定未涂层钢的相对早期耐溶解腐蚀性,并评估所选候选涂层(Cr $_2$ AlC、Al $_2$ O $_3$、V $_2$ Al $_x$ C $_y$)的保护性。钢的显微组织和热机械状态的预期差异的同时暴露显示钢的晶粒尺寸,退火/变形孪晶的密度,和二次析出物对钢的溶解腐蚀行为的影响。这项研究的结果提供了建议,钢铁制造的目的是使用钢建造第四代铅冷快堆。
Temperature and misorientation-dependent austenite nucleation at ferrite grain boundaries in a medium manganese steel: role of misorientation-dependent grain boundary segregation
In situ 2D visualization of hydrogen entry into Zn-coated steels in NaCl solutions: Roles of Zn dissolution and potential distribution
Institute for Materials Research, Tohoku University(东北大学材料科学研究所);Graduate School of Engineering, Tohoku University(东北大学研究生院工学研究科);Steel Research Laboratory, Nippon Steel Corporation(日本钢铁株式会社钢铁研究实验室)
HVAF Spraying of NiTi Coatings: Microstructure, Phase Transformation and Shape Memory Behavior
Institute of Physics of the Czech Academy of Sciences(捷克科学院物理研究所);Department of Engineering Science, University West(韦斯特大学工程科学系);Palacký University in Olomouc, Faculty of Science(奥洛穆茨帕拉茨基大学理学院);Joint Laboratory of Optics of Palacký University and Institute of Physics AS CR(帕拉茨基大学与捷克科学院物理研究所联合光学实验室);Oak Ridge National Laboratory(橡树岭国家实验室)