在500 $^\circ$ C下有和无防腐涂层的316 L和DIN奥氏体不锈钢在静态液态铅铋共晶(LBE)中的溶解腐蚀早期阶段
Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500$^\circ$C
摘要:
研究了316 L和DIN 1.4970奥氏体不锈钢与贫氧(C $_O$ < 10 $^-$ $^8$质量%)静态液态铅铋共晶(LBE)在500°C下接触600-1000 h后的溶解腐蚀行为的早期阶段($\le$ 1000 h)。本研究的目的是确定未涂层钢的相对早期耐溶解腐蚀性,并评估所选候选涂层(Cr $_2$ AlC、Al $_2$ O $_3$、V $_2$ Al $_x$ C $_y$)的保护性。钢的显微组织和热机械状态的预期差异的同时暴露显示钢的晶粒尺寸,退火/变形孪晶的密度,和二次析出物对钢的溶解腐蚀行为的影响。这项研究的结果提供了建议,钢铁制造的目的是使用钢建造第四代铅冷快堆。
英文摘要:
This work addresses the early stages ($\le$1000 h) of the dissolution corrosion behavior of 316L and DIN 1.4970 austenitic stainless steels in contact with oxygen-poor (C$_O$ < 10$^-$$^8$ mass%), static liquid lead-bismuth eutectic (LBE) at 500°C for 600-1000 h. The objective of this study was to determine the relative early-stage resistance of the uncoated steels to dissolution corrosion and to assess the protectiveness of select candidate coatings (Cr$_2$AlC, Al$_2$O$_3$, V$_2$Al$_x$C$_y$). The simultaneous exposure of steels with intended differences in microstructure and thermomechanical state showed the effects of steel grain size, density of annealing/deformation twins, and secondary precipitates on the steel dissolution corrosion behavior. The findings of this study provide recommendations on steel manufacturing with the aim of using the steels to construct Gen-IV lead-cooled fast reactors.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。