循环压缩下NiTi管材的功能退化和自增强弹性热冷却性能

Functional Degradation and Self-enhanced Elastocaloric Cooling Performance of NiTi Tubes under Cyclic Compression

Dingshan Liang, Peng Hua, Junyu Chen, Fuzeng Ren, Qingping Sun

摘要:

超弹性NiTi管是环保型弹性热冷却的有希望的候选者,但其循环稳定性受到功能退化的严重影响。在此,我们通过深入分析研究了纳米晶NiTi管的功能退化,并发现它有利于弹性热冷却性能。结果表明,功能退化伴随着残余应变的累积,滞后回线面积和相变应力显著减小。残余应变的积累来自于相变诱导的位错和位错钉扎的残余马氏体。前者将原始奥氏体晶粒分离成更小的纳米畴(相当于晶粒尺寸效应),并在相变过程中促进应变硬化,导致D.后者在奥氏体相中产生残余压应力,从而引起正相变应力的逐渐降低。因此,材料性能系数(COPmater)自增强为40~ 104%。其有益效果主要是由于D.该研究为定制COPmater和稳定NiTi的循环压缩力学响应提供了工艺路线。

英文摘要:

Superelastic NiTi tubes are promising candidates for eco-friendly elastocaloric cooling, but their cyclic stability suffers severely from functional degradation. Herein, we investigate the functional degradation of nanocrystalline NiTi tubes via in-depth analysis and find out that it is beneficial to elastocaloric cooling performance. The results show that the functional degradation accompanies with progressive accumulation of residual strain and significant reduction in both hysteresis loop area (D) and forward transformation stress. The accumulation of residual strain arises from phase-transition-induced dislocations and dislocation-pinned residual martensite. The former separates the original austenite grains to much smaller nanodomains (equivalent to grain size effect) and contributes to the strain hardening during phase transition, leading to the significant reduction of D. The latter induces compressive residual stress in the austenite phase and thus gives rise to the evolutive reduction of forward transformation stress. Consequently, the material coefficient of performance (COPmater) was self-enhanced for 40~104 %. The beneficial effect is mainly because of the cyclically-decreased D. The study might provide a processing route to tailor COPmater and stabilize the mechanical response of NiTi by cyclic compression.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑