局部表面缺陷对钝化接触太阳电池少子寿命的影响

Influence of local surface defects on the minority-carrier lifetime of passivating-contact solar cells

Jean Cattin, Jan Haschke, Christophe Ballif, Matthieu Boccard

摘要:

在硅太阳能电池行业中越来越流行的钝化接触的全部潜力的解锁,需要确定少数载流子寿命。微小的钝化压降会限制太阳能电池的功能,但是在开路电压低于700 mV的器件中不会检测到。在这项工作中,模拟和实验被用来显示局部表面缺陷对整体器件性能的影响。虽然缺陷没有显着影响电极沉积之前的寿命测量或开路电压测量在标准测试条件下,它有一个显着的影响点的操作,进而,器件效率(高达百分之几的效率下降)。此外,这项研究表明,局部缺陷可能会对通过电极的电连接位于几厘米远的钝化区域产生不利影响。这导致电极沉积后的低注入寿命下降。因此,通常在金属化之前测量的寿命曲线(以及因此内部电压)通常不代表金属化之后它们各自的值。在电极沉积之后经常观察到的低注入寿命下降可以源自这样的局部表面缺陷,而不是源自均匀钝化下降。

英文摘要:

Unlocking the full potential of passivating contacts, increasingly popular in the silicon solar cell industry, requires determining the minority carrier lifetime. Minor passivation drops limit the functioning of solar cells, however, they are not detected in devices with open-circuit voltages below 700 mV. In this work, simulations and experiments were used to show the effect of localized surface defects on the overall device performance. Although the defects did not significantly affect lifetime measurements prior to electrode deposition or open-circuit voltage measurements at standard-test conditions, it had a significant impact on the point of operation and, in turn, device efficiency (up to several percent efficiency drop). Furthermore, this study demonstrates that localized defects can have a detrimental effect on well-passivated areas located several centimeters away through electrical connection by the electrode. This leads to a low-injection lifetime drop after electrode deposition. Thus, commonly measured lifetime curves before metallization (and therefore internal voltage) are usually not representative of their respective values after metallization. The low-injection lifetime drop often observed after electrode deposition can derive from such local surface defects, and not from a homogeneous passivation drop.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑