掺铁beta-Ga2O3块体晶体红色发光的起源
On the origin of red luminescence from iron-doped beta-Ga2O3 bulk crystals
摘要:
目前,在~10^18 cm-3范围内的Fe掺杂是用于生产半绝缘单晶β-Ga 2 O3衬底的最广泛可用的方法。报道了多种Ga_2 O_3样品(包括Fe掺杂的Ga_2 O_3)的红色发光特性,并将其归因于O位的Fe或N。然而,在本文中,我们证明了来自Fe掺杂的β-Ga 2 O3商业衬底的高强度红色发光由在689 nm和697 nm处的两个尖锐峰叠加在以710 nm为中心的更宽的峰上组成,该高强度红色发光源自以接近2 ppm的浓度存在的Cr杂质。红色发射具有双重对称性,在吸收边附近的激发强度的峰值,似乎竞争与Ga 2 O 3发射在较高的激发能,并出现在Fe的存在下加强。基于偏振吸收、发光观察和Tanabe-Sugano图分析,我们提出了β-Ga_2 O_3基质中光生载流子与八面体配位的Cr ~(3+)的共振能量转移产生红色发光,并可能被Fe ~(3+)敏化。
英文摘要:
Currently, Fe doping in the ~10^18 cm-3 range is the most widely-available method for producing semi-insulating single crystalline beta-Ga2O3 substrates. Red luminescence features have been reported from multiple types of Ga2O3 samples including Fe-doped -Ga2O3, and attributed to Fe or N at O. Herein, however, we demonstrate that the high-intensity red luminescence from Fe-doped beta-Ga2O3 commercial substrates consisting of two sharp peaks at 689 nm and 697 nm superimposed on a broader peak centered at 710 nm originates from Cr impurities present at a concentration near 2 ppm. The red emission exhibits two-fold symmetry, peaks in intensity for excitation near absorption edge, seems to compete with Ga2O3 emission at higher excitation energy and appears to be intensified in the presence of Fe. Based on polarized absorption, luminescence observations and Tanabe-Sugano diagram analysis, we propose a resonant energy transfer of photogenerated carriers in beta-Ga2O3 matrix to octahedrally-coordinated Cr3+ to give red luminescence, possibly also sensitized by Fe3+.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。