纳米多孔石墨烯膜稳定性的热机械学洞察

Thermomechanical Insight into the Stability of Nanoporous Graphene Membranes

University of Brasília(巴西利亚大学)

Marcelo Lopes Pereira Junior, Luiz Antonio Ribeiro Junior

AI总结:

本研究通过ReaxFF分子动力学模拟,探究不同孔径的多孔n-Benzo-CMPs膜的力学与热稳定性,发现其热稳定温度低于石墨烯,断裂应变随孔径增大而升高,临界拉伸强度仅取决于孔径。

摘要:

多孔石墨烯(Porous graphene, PG)是一种具有纳米多孔结构的石墨烯衍生物。该材料拥有独特的结构,包含高孔体积的互连网络,可制备出具有大比表面积的膜。实验表明,PG兼具高机械强度、良好热稳定性等优异性能。本研究采用全原子反应性(ReaxFF,反应力场)分子动力学模拟,对具有不同纳米多孔结构的二维多孔n-Benzo-CMPs(CMP指π共轭微孔聚合物,n指孔径)膜的弹性能、断裂机制及热稳定性开展了全面研究。为便于对比,研究还将结果与相近尺寸的石墨烯片层结果进行了对照。我们采用了三种不同的纳米孔径:小(3.45 Å)、中(8.07 Å)、大(11.93 Å)。结果显示,PG在高达4660K的温度下仍保持热稳定,比石墨烯的熔点(5643K)低约1000K。在PG加热过程中,会形成由碳原子和氢原子组成的线性原子链。在温度不超过1200K的条件下,沿两个平面方向施加单轴载荷时,断裂应变范围为15%-34%,且断裂应变随纳米孔径的增大而成比例增加。值得注意的是,PG完全断裂的临界拉伸强度与温度无关,仅取决于纳米孔径。所有PG膜在达到临界应变阈值后,都会从弹性状态突然转变为完全断裂状态。

英文摘要:

Porous graphene (PG) is a graphene derivative endowed of nanoporous architectures. This material possesses a particular structure with interconnected networks of high pore volume, producing membranes with a large surface area. Experiments revealed that PG combines remarkable properties such as high mechanical strength and good thermal stability. In this work, we have carried out fully-atomistic reactive (ReaxFF) molecular dynamics simulations to perform a comprehensive study on the elastic properties, fracture mechanism, and thermal stability of 2D porous n-Benzo-CMPs (CMP and n refer, respectively, to pi-conjugated microporous polymers and the pore diameter) membranes with distinct nanoporous architectures. For comparison purposes, the results were also contrasted with the ones for graphene sheets of similar dimensions. We adopted three different nanoporous diameters: small (3.45 A), medium (8.07 A), and large (11.93 A). Results showed that PG is thermally stable up to 4660K, about 1000K smaller than the graphene melting point (5643K). During the PG heating, linear atomic chains are formed combining carbon and hydrogen atoms. The fracture strains range between 15%-34% by applying a uniaxial loading in both plane directions for temperatures up to 1200K. The fracture strain increases proportionally with the nanoporous size. Remarkably, the critical tensile strength for the PG complete fracture is temperature independent. Instead, it depends only on the nanoporous diameter. All the PG membranes go abruptly from elastic to completely fractured regimes after a critical strain threshold.