LiNiO2 has high energy density but easily reacts with moisture in the atmosphere and deteriorates. We performed qualitative and quantitative evaluations of the degraded phase of LiNiO2 and the influence of the structural change on the electrochemical properties of the phase. Li1-xHxNiO2 phase with cation exchange between Li+ and H+ was confirmed by thermogravimetric analysis and Karl Fischer titration measurement. As the H concentration in LiNiO2 increased, the rate capability deteriorated, especially in the low-temperature range and under low state of charge. Experimental and density functional theory (DFT) calculation results suggested that this outcome was due to increased activation energy of Li+ diffusion owing to cation exchange. Rietveld analysis of X-ray diffraction and DFT calculation confirmed that the c lattice parameter and Li-O layer reduced because of the Li+/H+ cation exchange. These results indicate that LiNiO2 modified in the atmosphere has a narrowed Li-O layer, which is the Li diffusion path, and the rate characteristics are degraded.
When supporting electrolyte matters - tuning capacitive response of graphene oxide via electrochemical reduction in alkali and alkaline earth metal chlorides
调节氧化石墨烯(GO)的电荷存储性质的能力对于能量转换应用是极其重要的。在这里,我们表明,GO的电化学还原对溶液中存在的阳离子高度敏感。GO在碱金属氯化物溶液中比在碱土金属氯化物中在更低的电势下被还原。在还原过程中,GO的电容从10倍增加到70倍。还原GO的最大电容在65和130 F g-1之间,这取决于电解质和导电添加剂的存在。我们建议,在还原过程中的阳离子与GO的氧官能团的不同的相互作用是负责所观察到的效果。
Free Energy Driven Transfer of Charge in Dense Electrochemically Active Monomolecular Films
对单分子膜作为电导体的兴趣源于对创新材料的探索。非共价键合的膜的效用是有限的,因为它们是机械不稳定的,并由不良连接域。因此,这些膜中的电荷转移被限制在微米量级的距离内。在这里,我们展示了最近开发的气相组装方法(Burtman,V.,Zelichenok,A.,Yitzchaik,S. 04 The Dog of the Dog(1999)Ed.38,2041-2045.),其产生共价连接到硅表面的坚固致密的NTCDI单层,允许人们克服这种规模限制。这些几乎绝缘的单层可以通过将电子喷射到半导体基底中而光化学地填充有阳离子自由基。阳离子自由基的正电荷可以在微秒内以随机游走的方式迁移远达几毫米,从而证明了膜的宏观连通性。由于电荷作为阳离子自由基存在,阳离子自由基是有效的氧化剂,因此它们的迁移与它们还原的自由能的转移相耦合,并且由氧化还原电势梯度驱动。阳离子自由基被阳极还原,将这种自由能转化为电动势。我们展示了这些薄膜如何可以实现在太阳能转换和基本的时间分辨的距离控制的研究序列的超快电子转移。
Influence of Ti/V Cation-Exchange in Na$_2$Ti$_3$O$_7$ on Na-Ion Negative Electrode Performance: an Insight from First-Principles Study
钛酸钠\ce{Na2Ti3O7}(NTO)被认为是一种非常有前途的负极材料,具有非常低的电压用于钠离子电池和电容器,但具有相对低的比容量和差的电子传导性。本文报道了NTO及其钒改性化合物\ce{Na2Ti2VO7}和\ce{Na2TiV2O7}(NTVO)的电化学性质的第一性原理研究,揭示了NTO及其钒改性化合物的详细工作机理,并为Ti/V阳离子交换提高阳极性能提供了依据。我们的计算表明,当使用\ce{NaTi_{3-$x$}V_{$x$}O7}($x$ = 1,2)作为Na插入的起始材料时,由于\ce{V^{+5}}的较高氧化态,以及较低的电压和小于3%的小体积膨胀率,比容量可以从NTO中的177 mAh g $^{-1}$增加到NTVO中的超过280 mAh g $^{-1}$。随着Ti/V交换,我们得到稍高的激活能Na离子迁移沿两个不同的途径,但发现一个明显的改善NTVO的电子输运。
Revealing the formation and electrochemical properties of bis(trifluoromethanesulfonyl) imide intercalated graphite with first-principles calculations
据报道,石墨作为双离子电池的阴极和阳极主体材料具有阴离子和阳离子嵌入能力。本文采用第一性原理计算研究了离子液体电解质中的二(三氟甲磺酰基)亚胺(TFSI)阴离子对石墨的插层作用。我们建立了TFSI-C $_n$化合物的模型,系统地增加石墨烯片的晶胞尺寸,并通过计算形成能来研究它们的稳定性,导致线性下降并达到稳定极限。通过确定形成稳定化合物的晶胞尺寸,我们发现TFSI-C $_n$的层间距和相对体积膨胀率随着TFSI插层浓度的增加而增加。在30 mAh g $^{-1}$至54 mAh g $^{-1}$的比容量范围内,电极电压被确定为在3.8 V至3.0 V的范围内,与实验一致。此外,TFSI迁移的50 meV以下的非常低的活化势垒和良好的电子导电性给出了使用这些化合物作为有前途的阴极的证据。通过对电荷转移过程的分析,阐明了TFSI-C $_n$的形成机理,为石墨基阴极材料的开发提供了新的前景。
Ni modified Fe3O4(001) surface as a simple model system for understanding the Oxygen Evolution Reaction
电化学水分解是一种以化学燃料的形式储存可再生能源的环保技术。在地球资源丰富的第一行过渡金属基催化剂中,Ni-Fe混合氧化物在碱性介质中有效且低成本地催化析氧反应(OER)方面表现出了良好的性能,但Fe和Ni阳离子在OER机理中的协同作用尚不清楚。在这项工作中,我们报告了添加Ni如何改变模型氧化铁催化剂的反应性,该模型氧化铁催化剂基于Ni沉积并结合在磁铁矿Fe 3 O 4(001)单晶中,使用超高真空中的表面科学技术的组合,如低能电子衍射(LEED)、X射线光电子能谱学(XPS)、低能离子散射(LEIS)、和扫描隧道显微镜(STM),以及在空气中的原子力显微镜(AFM),和电化学方法,例如循环伏安法(CV)和在碱性介质中的电化学阻抗谱(EIS)。当顶表面呈现20- 40%范围内的Fe:Ni组成比时,观察到OER活性的显著改善,这与对于粉末催化剂所观察到的良好一致。此外,在电解质中表面老化三天后,观察到OER过电位下降。在较高的Ni负载,AFM显示的增长归因于一个(氧)-氢氧化物相,根据CV测量,似乎不相关的表面活性对OER的一个新的阶段。EIS表明,OER前体物种上观察到的清洁和Ni改性的表面是相似的,Fe为中心,但形成在较低的过电位时,表面Fe:Ni的比例进行了优化。
Crystal structure, cobalt and iron speciation and oxygen non-stoichiometry of La0.6Sr0.4Co1-yFeyO3-d nanorods for IT-SOFC cathodes
Pontificia Universidad Javeriana(波哥大耶稣会天主教大学);Centro Atómico Constituyentes, Comisión Nacional de Energía Atómica(康塞普西翁原子中心,国家原子能委员会);Instituto de Nanociencia y Nanotecnología (INN), CNEA-CONICET(纳米科学与技术研究所,国家原子能委员会-国家科学研究和技术研究委员会);CONICET / Laboratorio de Cristalografía Aplicada, Escuela de Ciencia y Tecnología, Universidad Nacional de Gral. San Martín(国家科学研究和技术研究委员会/应用晶体学实验室,科学与科技学院,圣马丁国立大学);CNPEM, Laboratório Nacional de Luz Síncrotron(巴西纳米技术国家研究中心,同步光国家实验室);Instituto de Física, Universidade de São Paulo(物理研究所,圣保罗大学)