We computed the Compton profile of solid and liquid lithium using quantum Monte Carlo (QMC) and compared with recent experimental measurements obtaining good agreement. Importantly, we find it crucial to account for proper core-valence orthogonalization and to address density differences when comparing with experiment. To account for disorder effects, we sampled finite-temperature configurations using molecular dynamics (MD), then performed diffusion Monte Carlo (DMC) simulations on each configuration. We used Slater-Jastrow wavefunctions and grand-canonical twist-averaged boundary conditions. A QMC pseudopotential correction, derived from an all-electron DMC simulation of the perfect crystal was also used. Our calculations provide the first all-electron QMC benchmark for the Compton profile of lithium crystal and pseudopotential-corrected QMC Compton profiles for both the liquid and solid.
A Comparative Study of Molecular Dynamics Approaches for Simulating Ionic Conductivity in Solid Lithium Electrolytes
Université de Montréal(蒙特利尔大学);Mila – Quebec AI Institute(米拉-魁北克人工智能研究所);National Research Council Canada(加拿大国家研究委员会);Institut Courtois, Université de Montréal(蒙特利尔大学库尔图瓦研究所)
Measuring the buried interphase between solid electrolytes and lithium metal using neutrons
Oak Ridge National Laboratory(橡树岭国家实验室);Brookhaven National Laboratory(布鲁克海文国家实验室);Technical University Munich(慕尼黑工业大学);Czech Academy of Sciences(捷克科学院)
Evaluation and thermodynamic optimization of phase diagram of lithium niobate tantalate solid solutions
Leibniz-Institut für Kristallzüchtung (IKZ)(莱布尼茨晶体生长研究所);Institute of Applied Physics, Technische Universität Dresden(德累斯顿工业大学应用物理研究所);Paderborn University, Integrated Quantum Optics, Institute for Photonic Quantum Systems (PhoQS)(帕德博恩大学集成量子光学光子量子系统研究所)
Effect of lithium bis(oxalato)borate on the Structural, microstructural and electrochemical properties of blend solid polymer electrolyte
采用溶液浇铸法制备了以PEO、PVP为主体的锂离子复合聚合物电解质LiBOB,考察了LiBOB对聚合物电解质的形貌、结构和电化学性能的影响。XRD和FESEM分析表明,盐的加入提高了非晶含量。FTIR光谱证明了络合物的形成。优化体系的离子电导率比无盐体系高两个数量级,即~0.5x10-5 S cm-1(@RT),当O/Li=16时,提高到~0.65 mS cm-1(@100 oC),电导率随温度的变化符合Arrhenius性质。高的离子(~0.99)证明了络合电解质的离子性质。DSC分析表明,结晶度的抑制和玻璃熔融温度向低温移动意味着非晶含量的增加。最后,提出了一个相互作用机制,探索离子传输机制。本电解质体系可作为固态电池的潜在候选者
Interfacial Strain Effects on Lithium Diffusion Pathways in the Spinel Solid Electrolyte Li-Doped MgAl$_2$O$_4$
(Li,Al)共掺杂镁尖晶石(Li $_x$ Mg $_{1-2x}$ Al $_{2+x}$ O $_4$)是一种固体锂离子电解质,有可能用于全固态锂离子电池。与尖晶石电极(例如Li $_y$ Mn $_2$ O $_4$和Li $_{4+3z}$ Ti $_5$ O $_{12}$)的界面可以是晶格匹配的,具有潜在的低界面电阻。晶格匹配界面上的小晶格参数差异是不可避免的,导致残余外延应变。这种应变可能会改变界面附近的锂扩散,从而导致界面电阻。在这里,我们报告了一个密度泛函理论研究的应变影响的锂扩散途径(锂,铝)共掺杂镁尖晶石,$x_\mathrm{Li} = 0.25$和$x_\mathrm{Li} = 0.5$。我们已经计算了扩散分布的非应变材料,各向同性和双轴拉伸应变高达6%,对应于{100}外延界面与Li $_y$ Mn $_2$ O $_4$和Li $_{4+3z}$ Ti $_5$ O $_{12}$。我们发现,各向同性的拉伸应变减少锂扩散障碍多达0.32 eV,与典型的障碍减少约0.1 eV。这种效应与过渡八面体站点的体积增加有关,并且广泛地遵循局部静电势。对于双轴(外延)应变变化的八面体网站的体积和锂扩散障碍比各向同性应变小得多。典型的势垒仅降低~ 0.05 eV。然而,个体效应取决于所考虑的途径和相对应变方向。这些结果预测,各向同性应变强烈影响离子电导率(Li,…
A Fibrous Solid Electrolyte for Lithium-ion Batteries
在这项工作中提出的新方法使用氧化物细丝/纤维代替致密的薄膜电解质,从而允许:(i)直接制造而不使用昂贵的薄膜生产技术,(ii)现有锂离子电池生产线的微小变化,以及(iii)更好的机械稳定性和电化学性能。采用静电纺丝技术制备了Li 7 La 3 Zr 2 O 12(LLZO)纤维作为电解质。利用X射线衍射(XRD)和扫描电镜(SEM)对产物的物相和形貌进行了表征。结果表明,所制备的电解液在电池安全性和性能方面是电动汽车用全固态电池的良好替代品。
X射线吸收光谱(XAS)是材料表征的首要技术,提供有关吸收体原子局部化学环境的关键信息。在这项工作中,我们开发了一个数据库的硫K边XAS光谱的结晶和非晶硫代磷酸锂材料的原子结构的基础上报告的化学材料,34,6702(2022)。XAS数据库是基于使用维也纳从头算模拟包中实现的激发电子和芯孔赝势方法的模拟。我们的数据库包含66个晶体和玻璃结构模型的2681 S K边XAS光谱,使其成为迄今为止玻璃/陶瓷硫代磷酸锂的第一原理计算XAS光谱的最大集合。该数据库可用于关联S光谱特征与不同的S物种的基础上,他们的本地协调和短程有序的硫化物为基础的固体电解质。这些数据通过材料云公开分发,允许研究人员免费访问并用于进一步分析,例如光谱指纹,与实验匹配和开发机器学习模型。
Particle Morphology and Lithium Segregation to Surfaces of the Li$_7$La$_3$Zr$_2$O$_{12}$ Solid Electrolyte
用于固态锂离子电池的固体电解质激发了对下一代能量存储应用的极大兴趣。Li $_7$ La $_3$ Zr $_2$ O $_{12}$石榴石型固体电解质由于其高离子电导率而受到相当大的关注。然而,基于Li $_7$ La $_3$ Zr $_2$ O $_{12}$的固态器件的成功应用仍然存在若干挑战,例如枝晶形成和在许多Li嵌入/提取循环中保持界面处的物理接触。在这里,我们应用第一性原理密度泛函理论提供的见解,在各种物理和化学条件下的Li $_7$ La $_3$ Zr $_2$ O $_{12}$粒子形态。我们的研究结果表明,锂偏析的表面,建议富锂晶界在典型的合成和烧结条件。我们的研究结果的基础上,我们提出了切实可行的策略,以遏制Li $_7$ La $_3$ Zr $_2$ O $_{12}$接口的Li偏析。这种方法可以扩展到其他锂离子导体的实际储能装置的设计。
Machine-Learning-Guided Insights into Solid-Electrolyte Interphase Conductivity: Are Amorphous Lithium Fluorophosphates the Key?
Bakar Institute of Digital Materials for the Planet, UC Berkeley(加州大学伯克利分校巴卡尔数字材料行星研究所);Materials Sciences Division, Lawrence Berkeley National Laboratory(劳伦斯伯克利国家实验室材料科学部);Department of Materials Science and Engineering, National University of Singapore(新加坡国立大学材料科学与工程系)
Are Weakly Coordinating Anions Really the Holy Grail of Ternary Solid Polymer Electrolytes Plasticized by Ionic Liquids? Coordinating Anions to the Rescue of the Lithium Ion Mobility
Direct observation of reversible ionic polarization at a buried solid-state battery interface
Nuclear Physics Institute of Czech Academy of Sciences(捷克科学院核物理研究所);Slovak University of Technology in Bratislava(布拉迪斯拉发斯洛伐克理工大学);SRM University-AP(SRM大学安得拉邦分校);CNR-ITAE(意大利国家研究委员会离子技术及应用研究所);University of Messina(墨西拿大学)
Flexible, solid electrolyte-based lithium battery composed of LiFePO4 cathode and Li4Ti5O10 anode for applications in smart textiles
在这里,我们报告制造的灵活和可拉伸的电池组成的应变自由LiFePO 4阴极,Li 4 Ti 5 O 10阳极和固体聚环氧乙烷(PEO)电解质作为隔膜层。该电池是从智能纺织品应用的角度开发的。该电池以固体热塑性电解质为关键使能元件,可挤压或拉伸成纤维或细条,直接与智能纺织品制造中使用的编织工艺兼容。本文首先详细介绍了材料的选择,电极和隔膜层的制造和表征。然后组装电池并对其进行表征,最后,将由几个长条制成的大型电池样品编织成织物,用导电线连接,并进行表征。在本文中,我们详细研究了电池设计的两个实际方面:第一是以导电碳和聚合物粘合剂材料的优化比例制备阴极/阳极材料的复合材料,第二是电池性能,包括循环,可逆性和阴极/阳极材料的相容性。最后,当铸造电极和隔膜层时,我们主要关注使用水溶液代替有机溶剂,以使制造过程环境友好。
Pseudo-ternary LiBH4-LiCl-P2S5 system as structurally disordered bulk electrolyte for all-solid-state lithium batteries
研究了LiBH_4-LiCl-P_2S_5混合体系在全固态电池中的性能。所研究的材料在加热到601 ℃以上时发生非晶化,伴随着有利于电池电解质应用的Li+电导率增加。在室温下测得的离子电导率为10- 3Scm-1,非晶化后的激活能为0.40(2)eV。材料的结构分析和表征表明,BH 4基团和PS 4可能属于相同的分子结构,其中Cl离子相互作用以容纳结构单元。由于其导电性,延展性和电化学稳定性(高达5 V,Au vs. Li+/Li),这种新的电解质在使用阴极材料(层状TiS 2,theo.在501 ℃下,以Li为阳极,在12 mA g ~(-1)(0. 05 C-倍率)的电流密度下进行10次循环,容量保持率为93%,循环稳定性良好。通过透射模式的同步加速器X射线衍射进行的进一步先进表征明显有助于更好地了解在中等温度下运行的固态电池电极的(脱)锂过程。
From anti-perovskite to double anti-perovskite: lattice chemistry basis for super-fast transportation of Li+ ions in cubic solid lithium halogen-chalcogenides
Li4-xGe1-xPxO4 a potential solid-state electrolyte for all-oxide microbatteries
用于锂离子电池的固态电解质正引起越来越多的关注,因为它们可以制造更安全的电池,也可以使用锂金属阳极。本文研究了锂超离子导体(LISICON)家族中的一种化合物,即Li_(4-x)Ge_(1-x)P_xO_4(LGPO)。通过脉冲激光沉积来沉积薄膜,并将其电性能与陶瓷颗粒进行比较。微观结构的详细表征表明,薄膜可以在较高的温度下沉积完全结晶,但在室温下也可以部分非晶。电导率不会受到晶界存在、暴露于空气或锂不足的强烈影响。采用第一性原理分子动力学模拟计算了理想LGPO晶体在不同温度下的锂离子扩散分布和电导率。模拟给出了无缺陷晶体的电导率上限,在300 ℃时为10-2 S cm-1。薄膜制备的容易性、在几μ S cm-1范围内的室温Li离子电导率使得LGPO成为用于薄膜全固态全氧化物微电池的非常有吸引力的电解质材料。