Ba(Fe $_{1-x}$ Co $_{x}$)$_{2}$ As $_{2}$滞弹性畴弛豫的电阻率调制研究

Signatures of Anelastic Domain Relaxation in Ba(Fe$_{1-x}$Co$_{x}$)$_{2}$As$_{2}$ Investigated by Mechanical Modulation of Resistivity

Alexander T. Hristov, Matthias S. Ikeda, Johanna C. Palmstrom, Ian R. Fisher

摘要:

研究了Ba(Fe $_{1-x}$ Co $_{x}$)$_{2}$ As $_{2}$在多畴状态下对交流机械形变的电阻响应。这种电阻变化既取决于畴壁的滞弹性弛豫,也取决于电阻与畴壁构型之间的关系。将样品粘附到压电堆的表面,压电堆由AC电压驱动,同时测量样品电阻的AC调制。由于电子的响应时间比晶格的响应时间快,所以压电体的AC电阻调制和AC变形之间的相位差$ϕ$完全是由于样品中的滞弹性弛豫效应。在这个实验配置中,推导出用于将$ϕ$与样品的复杂顺应性$J(ω)$相关联的表达式。对Ba(Fe $_{1-x}$ Co $_{x}$)$_{2}$ As $_{2}$(x=(0.025,0.052))的测量表明,在正交反铁磁态中,异相电阻率调制的峰值远低于Neél温度$T_N$和结构转变$T_S$。同时,对于在所有温度下都是四方晶系的组合物,x=0.07,电阻调制在相同温度下保持完全同相,建立畴运动作为在经历四方晶系到正交晶系转变的样品中观察到的效应的可能原因。拟合的$\tanϕ$的样品与x=0.025的压电叠层上的各种振幅的激励,从其中畴壁运动的表观激活能$E_a$被发现,以减少沿$[110]_T$轴的变形的幅度增加。我们发现$\frac{dE_a}{d\varepsilon^0_{[110,110]_T}} = -1115\pm 196$ eV与$E_a = 9.09 \pm 0.74 \times 10^{-3}$ eV在零应变极限,如果我们假设在整个范围内的应变振幅的线性。

英文摘要:

The resistive response of Ba(Fe$_{1-x}$Co$_{x}$)$_{2}$As$_{2}$ to AC mechanical deformation is considered in the multi-domain state. This resistance change depends both upon the anelastic relaxation of domain walls and upon the relation between resistance and the domain wall configuration. Samples are adhered to the surface of a piezoelectric stack, which is driven by an AC voltage while the AC modulation of the sample resistance is measured. As the response time of electrons is faster than that of the lattice, the phase difference $ϕ$ between the AC resistance modulation and the AC deformation of the piezoelectric is entirely due to anelastic relaxation effects in the sample. An expression is derived for relating $ϕ$ to a sample's complex compliance, $J(ω)$, in this experimental configuration. Measurements of Ba(Fe$_{1-x}$Co$_{x}$)$_{2}$As$_{2}$ for x= (0.025, 0.052) reveal a peak in the out-of-phase resistivity modulation in the orthorhombic antiferromagnetic state well below the Neél temperature $T_N$ and structural transition $T_S$. Meanwhile, for a composition that is tetragonal at all temperatures, x=0.07, the resistance modulation remains entirely in phase over the same temperatures, establishing domain motion as a probable cause of the observed effects in the samples that do undergo the tetragonal-to-orthorhombic transition. Fits are provided of $\tanϕ$ for a sample with x=0.025 for various amplitude excitations on the piezoelectric stack, from which the apparent activation energy $E_a$ for domain wall motion is found to decreases with increasing amplitude of the deformation along the $[110]_T$ axis. We find $\frac{dE_a}{d\varepsilon^0_{[110,110]_T}} = -1115\pm 196$ eV with $E_a = 9.09 \pm 0.74 \times 10^{-3}$ eV in the zero strain limit if we assume linearity over the entire range of strain amplitudes.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑