arXiv 1810.00899cond-mat.mtrl-sciphysics.app-ph
收藏

氧化铟钝化ZnO(0001)表面的同步辐射光电子能谱研究

Synchrotron radiation based photoemission studies of indium oxide passivation of ZnO(0001) surface at high temperature

Kumarappan Kumar, Greg Hughes

摘要:

通过原位沉积金属铟和沉积后高温(600 C - 1000 C)退火来进行表面活性ZnO(0001)-Zn终止表面的钝化。在铟沉积和退火的每个循环之后,ZnO(0001)表面的特征在于基于同步辐射的光电发射。光电发射研究证实了沉积铟的形成转化为氧化铟(In 2 O3和In 2 Ox)作为表面钝化层。为了提高表面灵敏度,在不同的光子能量下获得了Zn、C、O的芯能级谱。总体芯能级峰(Zn 3 p,In 4d,O 1 s)具有范围从0.5 eV至0.8 eV的平均结合位移。价带谱表明,钝化后的薄膜费米能级位移为0.9eV,功函数从4.06eV提高到4.77eV。氧化铟高温钝化使ZnO(0001)表面的能带向下弯曲变为向上弯曲0.98eV,适合于制作ZnO肖特基接触和器件。

英文摘要:

Passivation of surface reactive ZnO(0001)-Zn terminated surface is carried out by in-situ deposition of indium metal and post deposition annealing at high temperature (600 C - 1000 C). After the every cycle of indium deposition and annealing the ZnO(0001) surface is characterised by synchrotron radiation based photoemission. The photoemission studies confirmed the formation of deposited indium turned into indium oxide (In2O3 and In2Ox) as surface passivation layer. The core level spectra for Zn, C, O, were acquired at different photon energy for high surface sensitivity. Overall core level peaks (Zn 3p, In 4d, O 1s) having average binding shift ranging from 0.5 eV to 0.8 eV. The valance band spectra shows fermi level shift of 0.9 eV after passivation at 1000 C and work function raises form 4.06 eV to 4.77 eV. Downward band bending of ZnO(0001) surface is turned into upward bending of 0.98 eV by indium oxide passivation at high temperature, which is suitable for making ZnO schotty contact and devices.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑