arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1802.08423cond-mat.mtrl-sci
收藏

钙钛矿氧化物表面热制备过程中表面形态和重构的独立性

Independence of surface morphology and reconstruction during the thermal preparation of perovskite oxide surfaces

Maren Jäger, Ali Teker, Jochen Mannhart, Wolfgang Braun

摘要:

使用CO $_2$激光器从背面直接加热晶体,可以原位热制备SrTiO $_3$衬底用于外延,而不需要非原位蚀刻和退火。我们发现,在900-1100 °C下形成具有直台阶的大平台与外延的理想表面重构的形成无关,这需要超过1200 °C的温度才能完成。该方法可以是通用的,至少对于钙钛矿氧化物表面是通用的,因为它在不同温度下也适用于LaAlO $_3$和NdGaO $_3$,这两种其它广泛使用的氧化物衬底材料。

英文摘要:

Using a CO$_2$ laser to directly heat the crystals from the back side, SrTiO$_3$ substrates may be thermally prepared in situ for epitaxy without the need for ex-situ etching and annealing. We find that the formation of large terraces with straight steps at 900-1100 °C is independent from the formation of the ideal surface reconstruction for epitaxy, which requires temperatures in excess of 1200 °C to complete. The process may be universal, at least for perovskite oxide surfaces, as it also works, at different temperatures, for LaAlO$_3$ and NdGaO$_3$, two other widely used oxide substrate materials.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑