基于InAlN/GaN-on-Si HEMT堆栈的UV探测器,光暗电流比> 107

UV Detector based on InAlN/GaN-on-Si HEMT Stack with Photo-to-Dark Current Ratio > 107

Sandeep Kumar, Anamika Singh Pratiyush, Surani Bin Dolmanan, Sudhiranjan Tripathy, Rangarajan Muralidharan, Digbijoy Neelim Nath

摘要:

我们展示了一种基于InAlN/GaN-on-Si HEMT的紫外探测器,其光暗电流比大于107。Ti/Al/Ni/Au金属叠层被蒸发并快速热退火,用于在InAlN/GAN界面处与2D电子气(2DEG)的欧姆接触,同时沟道+势垒被凹陷蚀刻至20 nm的深度以夹断源极-漏极焊盘之间的2DEG。在5 V电压下测量的367 nm处的光谱响应度(SR)为34 A/W,光暗电流比非常高,> 10^7。发现在固定偏压下的光暗电流比随着PD的凹槽长度的增加而减小。所制造的器件被发现表现出紫外-可见光抑制比>103与低暗电流< 32 pA,在5 V的瞬态测量显示上升和下降时间在3-4 ms的范围内。增益机制进行了研究,估计载流子寿命与其他地方报道的匹配良好。

英文摘要:

We demonstrate an InAlN/GaN-on-Si HEMT based UV detector with photo to dark current ratio > 107. Ti/Al/Ni/Au metal stack was evaporated and rapid thermal annealed for Ohmic contacts to the 2D electron gas (2DEG) at the InAlN/GaN interface while the channel + barrier was recess etched to a depth of 20 nm to pinch-off the 2DEG between Source-Drain pads. Spectral responsivity (SR) of 34 A/W at 367 nm was measured at 5 V in conjunction with very high photo to dark current ratio of > 10^7. The photo to dark current ratio at a fixed bias was found to be decreasing with increase in recess length of the PD. The fabricated devices were found to exhibit a UV-to-visible rejection ratio of >103 with a low dark current < 32 pA at 5 V. Transient measurements showed rise and fall times in the range of 3-4 ms. The gain mechanism was investigated and carrier lifetimes were estimated which matched well with those reported elsewhere.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑