arXiv 1707.00217cond-mat.mtrl-sci
收藏

IV族半导体(Si,Ge)中Mn纳米线和团簇作为δ掺杂层的磁性

Magnetism in Mn Nanowires and Clusters as δ-doped Layers in Group IV Semiconductors (Si, Ge)

K. R. Simov, P. -A. Glans, C. A. Jenkins, M. Liberati, P. Reinke1

摘要:

IV族半导体(Si/Ge)的Mn掺杂是通过在IV族基质中嵌入薄Mn膜作为δ掺杂层来实现的。Mn层由单原子Mn线的致密层组成,其垂直于Si(001)-(2x 1)二聚体行或Mn簇定向。纳米结构覆盖有非晶Si或Ge覆盖层,这保留了δ掺杂层的特性。与STM的键合环境的分析相结合的元素特定的检测与X射线磁性圆二色性的磁性签名。具有离子键特性的Mn线在a-Ge覆盖层上的磁矩最大(2.5 μB/Mn),a-Si覆盖层导致磁矩略有降低,这是由于键几何结构的细微变化。我们的结果直接证实了Mn吸附在Si(001)表面的磁性理论预测。δ掺杂层的磁矩淬灭到0.5μB/Mn,主要由团簇组成,从而形成Mn-Mn键的反铁磁成分。

英文摘要:

Mn doping of group-IV semiconductors (Si/Ge) is achieved by embedding a thin Mn-film as a δ-doped layer in group-IV matrix. The Mn-layer consists of a dense layer of monoatomic Mn-wires, which are oriented perpendicular to the Si(001)-(2x1) dimer rows, or Mn-clusters. The nanostructures are covered with an amorphous Si or Ge capping layer, which conserves the identity of the δ-doped layer. The analysis of the bonding environment with STM is combined with the element-specific detection of the magnetic signature with X-ray magnetic circular dichroism. The largest moment (2.5 μB/Mn) is measured for Mn-wires, which have ionic bonding character, with an a-Ge overlayer cap, a-Si capping leads to a slightly reduced moment which has its origin in subtle variation of bonding geometry. Our results directly confirm theoretical predictions on magnetism for Mn-adatoms on Si(001). The moment is quenched to 0.5μB/Mn for δ-doped layers, which are dominated by clusters, and thus develop an antiferromagnetic component from Mn-Mn bonding.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑