We report on the thermally activated flux flow dependency on the doping dependent mixed state in NaFe1-xCoxAs (x=0.01, 0.03, and 0.07) crystals using the magnetoresistivity in the case of B//c-axis and B//ab-plane. It was found clearly that irrespective of the doping ratio, magnetoresistivity showed a distinct tail just above the Tc, offset associated with the thermally activated flux flow (TAFF) in our crystals. Furthermore, in TAFF region the temperature dependence of the activation energy follows the relation U(T, B)=U_0 (B) (1-T/T_c )^q with q=1.5 in all studied crystals. The magnetic field dependence of the activation energy follows a power law of U_0 (B)~B^(-α) where the exponent α is changed from a low value to a high value at a crossover field of B=~2T, indicating the transition from collective to plastic pinning in the crystals. Finally, it is suggested that the 3D vortex phase is the dominant phase in the low-temperature region as compared to the TAFF region in our series samples.
Magnetic field dependence of vortex activation energy: a comparison between MgB2, NbSe2 and Bi2Sr2Ca2Cu3O10 superconductors
在低电流密度下的耗散机制进行了比较,在三个不同类别的超导体。这是通过测量作为温度和磁场的函数的电阻,在干净的NbSe 2,MgB 2和Bi 2 Sr 2 Ca 2 Cu 3 O 10超导体的多晶样品。热激活磁通流动行为清楚地确定在散装硼化镁。虽然MgB2在低场下的激活能与Bi2Sr2Ca2Cu3O10相当,但其场依赖性遵循抛物线行为,与Bi2Sr2Ca2Cu3O10中看到的幂律依赖性不同。我们分析了我们的结果的基础上的Kramer的缩放晶界钉扎在MgB2和NbSe2。
Plastic vortex-creep in YBa$_2$Cu$_3$O$_{7-x}$ crystals
在$_2$ $_3$ O $_{7-x}$晶体中的局部磁弛豫测量显示与在涡旋晶格中的位错的运动相关联的塑性涡旋蠕变的证据。这种蠕变机制支配着在宽范围的温度和低于熔化线和高于对应于“鱼尾”磁化峰的磁场的磁场中的涡旋动力学。在此范围内,随电场减小的活化能$U_{pl}$下降到低于随电场增大的弹性(集体)蠕变活化能$U_{el}$。磁通动力学从弹性蠕变到塑性蠕变的交叉被证明是YBa $_2$ Cu $_3$ O $_{7-x}$中鱼尾的起源。
Vortex Lattice Melting into Disentangled Liquid Followed by the 3D-2D Decoupling Transition in YBa_2Cu_4O_8 Single Crystals
在高质量的YBa_2Cu_4O_8单晶中观察到与涡旋晶格熔化有关的急剧电阻降。各向异性GL理论很好地描述了熔化线。在涡旋液相中观察到两个热激活磁通流区,它们被一条相交线B_cr=1406.5(1-T/T_c)/T(T_c=79.0 K,B_cr in T)分隔开。得到了各个区域的激活能,并讨论了相应的耗散机制。结果表明,YBa_2Cu_4O_8单晶中的涡旋晶格熔化为解纠缠的液体,然后发生3D-2D退耦转变。
Comparative study of vortex dynamics in CaKFe4As4 and Ba0.6K0.4Fe2As2 single crystals
本文研究了两种典型的空穴掺杂铁基超导体CaKFe $_4$ As $_4$(CaK 1144)和Ba $_{0.6}$ K $_{0.4}$ Fe $_2$ As $_2$(BaK 122)中的涡旋动力学。发现BaK 122的磁滞回线在较宽的温度范围内具有明显的第二峰效应,而CaK 1144的磁滞回线则不存在第二峰效应。然而,在CaK 1144中观察到临界电流密度与温度的第二峰值效应,然而在BaK 122中不存在该效应。BaK 122和CaK 1144中第二峰效应的不同表现可能暗示了不同体系中涡旋钉扎的不同起源。磁化强度和它的松弛也被测量通过使用动态和传统的松弛方法为两个系统。通过对两种不同体系的分析和比较,发现BaK 122体系的涡旋钉扎更强,临界电流密度更高。发现Maley方法可以用于BaK_(122)体系,从而可以在较宽的温度范围内利用随时间变化的磁化强度来确定活化能,但这不适用于CaK_(1144)体系。最后,我们提出了不同的制度与不同的涡动力学的场-温度图为两个系统。
Flux-flow and vortex-glass phase in iron pnictide BaFe$_{2-x}$Ni$_x$As$_2$ single crystals with $T_c$ $\sim$ 20 K
我们分析了三种晶体BaFe $_{2-x}$ Ni $_x$ As $_2$与$T_c$ $\sim$ 20 K三种不同的几何形状相对于所施加的磁场和晶体的c轴之间形成的角度的等场磁电阻率数据的磁通流区域。场依赖的活化能,$U_0$,从TAFF和修改后的涡旋玻璃模型,这是比较从磁通蠕变文献中获得的$U_0$的值。我们观察到由TAFF模型得到的$U_0$在不同的晶体之间显示出偏差,而由涡旋玻璃模型得到的相应的玻璃线几乎是一致的。它示出的数据是很好地解释了修改后的涡旋玻璃模型,允许提取值的$T_g$,玻璃化转变温度,和$T^*$,温度与平均场临界温度$T_c(H)$的规模。所得到的玻璃线服从各向异性的金兹伯格-朗道理论,并很好地拟合在文献中发展的理论,考虑到无序的影响。
Collective vortex pinning and crossover between second order to first order transition in optimally doped Ba1-xKxBiO3 single crystals
对最佳掺杂的Ba $_{0.59}$ K $_{0.47}$ Bi O $_{3+δ}$单晶($T_c$ = 31.3 K)进行了磁化和弛豫测量。对数据进行了详细分析。动态弛豫和常规弛豫已被测量导致的磁化弛豫速率的自洽的确定。结果表明,在磁场为1和3 T时,样品的玻璃化指数约为$μ\approx$ 1.64 ~ 1.68,符合集体钉扎模型。基于Maley方法的分析结合常规弛豫数据使我们能够确定与电流相关的激活能$U$,对于1和3 T的磁场,其产生的$μ$值约为1.23至1.29。第二磁化峰出现在2 ~ 24 K的宽温区。第二峰值场与不可逆场之间的距离随着温度的升高而变窄。当两个场相互靠近时,第二个峰演变成一个阶梯状的磁化转变,表明存在从二级到一级的过渡。最后,我们给出了一个涡旋相图,并证明了在Ba $_{1-x}$ K $_x$ Bi O $_3$中的涡旋动力学可以用作研究集体涡旋钉扎的模型系统。
Vortex dynamics as a function of field orientation in BaFe1.9Ni0.1As2
多带各向异性超导体(如铁基超导体)中的涡旋动力学是一个有趣的问题,具有潜在的应用价值。在这项研究中,我们检查磁通蠕变数据沿第二磁化峰观察到的M(H)曲线BaFe $_{1.9}$ Ni $_{0.1}$作为$_2$ H//c轴,H//ab $-planes and H forming a 45$ ^o$角ab平面。我们发现,从不同的磁场方向采取的M-H环可以塌缩到一个单一的通用曲线在所有温度下与一个简单的比例因子相当于超导各向异性,不仅表明,涡旋钉扎是各向同性的,三维的,最有可能与点状缺陷。然而,所得到的临界电流,采取从Bean模型似乎显示出增强的低场钉扎H//c。涡旋动力学中的特征在不同的场取向中也不同,并且不显示与第二磁化峰Hp的直接相关性,如在钉扎机制中具有直接交叉的情况。从磁通蠕变数据得到的缩放激活能的等场图被发现是一个光滑的温度函数的Hp(T)线是交叉一致的一个单一类型的钉扎制度在这个领域的操作,独立的字段方向。结果相图中Hp(T)线的函数形式也支持这一观点。
Vortex creep and critical current densities in superconducting (Ba,K)Fe$_{2}$As$_{2}$ single crystals
研究了在平行于c轴和$ab$ -平面的磁场作用下,Ba $_{1-x}$ K $_{x}$ Fe $_{2}$ As $_{2}$单晶临界态的可持续电流密度的惊人的快速弛豫.针对高温超导铜氧化物磁通蠕变的标准分析方法的不足,提出了一种简单、直观的数据处理方法,揭示了高温超导铜氧化物磁通蠕变的机理和蠕变指数$μ$。在低磁场下,低于第二磁化峰,$μ$仅作为温度和磁通量密度$B$的函数略微变化。从数据中,我们确定的温度和场的依赖性的有效激活势垒蠕变。在低温下,测得的电流密度接近零-温度临界电流密度(在蠕变的情况下)的一个因素2内,从而贷款的可信度,以较早的结论得出的钉扎机制。实验屏蔽电流密度和零温临界电流密度的可比值揭示了广泛使用的“插值公式”的有限用途。
Crystal structure effects on vortex dynamics in superconducting MgB$_2$ thin films
University of Vienna(维也纳大学);Technische Universität Braunschweig(布伦瑞克工业大学);Institute Jean Lamour, Université de Lorraine-CNRS(洛林大学-法国国家科学研究中心让·拉穆尔研究所);G.V. Kurdyumov Institute for Metal Physics of the NAS of Ukraine(乌克兰国家科学院G.V.库尔久莫夫金属物理研究所);FLUXONICS—The European Foundry for Superconducting Electronics e.V.(FLUXONICS——欧洲超导电子铸造协会)