单层和少层WTe2纳米片的环境不稳定性及其降解
Environmental Instability and Degradation of Single- and Few-Layer WTe2 Nanosheets in Ambient Conditions
摘要:
由于发现大的,非饱和的磁阻在散装WTe 2,允许微剥离,单层和少层WTe 2晶体吸引了越来越多的兴趣。然而,正如现有研究中提到的,WTe2薄片似乎在环境条件下降解。在这里,我们报告的实验观察饱和退化在几层WTe2通过拉曼光谱表征和仔细监测的退化的单层,双层和三层(1L,2L和3L)WTe2在很长一段时间。拉曼峰强度在WTe2降解过程中降低,并且1L薄片比2L和3L薄片降解更快。在1L WTe2中的相对较快的降解可归因于与WTe2的氧反应的低能垒。利用XPS和AES进一步研究了WTe2的降解机理,发现Te和W原子的氧化是WTe2降解的主要原因。此外,我们观察到氧化仅发生在靠近表面的0.5nm深度处,并且氧化的WTe 2表面可以帮助防止内层进一步退化。
英文摘要:
Since the discovery of large, non-saturating magnetoresistance in bulk WTe2 which allows microexfoliation, single- and few-layer WTe2 crystals have attracted increasing interests. However, as it mentioned in existing studies, WTe2 flakes appear to degrade in ambient conditions. Here we report experimental observations of saturating degradation in few-layer WTe2 through Raman spectroscopy characterization and careful monitoring of the degradation of single-, bi- and tri-layer (1L, 2L & 3L) WTe2 over long time. Raman peak intensity decreases during WTe2 degradation and 1L flakes degrade faster than 2L and 3L flakes. The relatively faster degradation in 1L WTe2 could be attributed to low energy barrier of oxygen reaction with WTe2. We further investigate the degradation mechanisms of WTe2 using XPS and AES and find that oxidation of Te and W atoms is the main reason of WTe2 degradation. In addition, we observe oxidation occurs only in the depth of 0.5nm near the surface, and the oxidized WTe2 surface could help prevent inner layers from further degradation.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。