在这项工作中,分子力学模拟使用改进的嵌入原子方法(MEAM)的潜力,以产生一系列的正烷烃分子从乙烷(C $_2$ H $_6$)十一烷(n-C $_{11}$ H $_{24}$)在拉伸变形到键断裂点的应力-应变响应。结果进一步推广到一个单一的聚乙烯(PE)链。力、真实柯西应力、真实维里应力和杨氏模量被计算为所有分子的真实应变的函数。在计算单个分子的应力时,基于三种不同的度量建议了三种方法(在本工作中指定为M1、M2和M3)来量化变形期间的瞬时分子横截面积和体积。这些方法的预测相比,理论,第一原理,和实验数据。M1给出了真正的柯西应力和真正的维里应力结果,它们基本上是等效的,这表明它是计算烷烃分子应力的更好方法,因此,PE单链。使用M1、M2和M3的单个PE链的平均弹性模量的MEAM预测分别为401 GPa、172 GPa和147 GPa。虽然这些结果是不同的,但M1给出的模量值与PE的-CH $_2$ CH $_2$ -重复单元在0 K下的从头计算值405 GPa惊人地接近。为了进一步测试MEAM势,计算正交PE晶胞的杨氏模量(C $_{33}$弹性常数),但是其值(184 GPa)比DFT计算值316 GPa低估42%。
英文摘要:
In this work, molecular mechanics simulations were performed using a modified embedded-atom method (MEAM) potential to generate the stress-strain responses of a series of n-alkane molecules from ethane (C$_2$H$_6$) to undecane (n-C$_{11}$H$_{24}$) in tensile deformation up to the point of bond rupture. The results are further generalized to a single polyethylene (PE) chain. Force, true Cauchy stress, true virial stress, and Young's moduli were calculated as a function of true strain for all of the molecules. In calculating the stress of a single molecule, three methods (designated in this work as M1, M2, and M3) are suggested based on three different metrics to quantify both the instantaneous molecular cross-sectional area and volume during deformation. The predictions of these methods are compared to theoretical, first-principles, and experimental data. M1 gives true Cauchy and true virial stress results that are essentially equivalent, suggesting that it is a better method for calculating stress in alkane molecules and, hence, PE single chain. The MEAM predictions of the average elastic modulus for a single PE chain using M1, M2, and M3 are 401 GPa, 172 GPa, and 147 GPa, respectively. Though these results are disparate, M1 gives a modulus value that is strikingly close to the ab initio-calculated value of 405 GPa for the -CH$_2$CH$_2$- repeat unit of PE at 0 K. To further test the MEAM potential, the Young's modulus (C$_{33}$ elastic constant) of an orthorhombic PE crystal cell was calculated, but its value (184 GPa) underestimates the DFT-calculated value of 316 GPa by 42%.
Polyethylene under tensile load: strain energy storage and breaking of linear and knotted alkanes probed by first-principles molecular dynamics calculations
On the elastic moduli of three-dimensional assemblies of spheres: characterization and modeling of fluctuations in the particle displacement and rotation
Rheological constitutive equation for model of soft glassy materials
我们精确地求解并详细地描述了泡沫、乳状液、泥浆等的低频剪切流变学的简化标量模型。Lequeux,P. Hebraud,M. E. Cates,Phys. Rev. Lett. 78,2020(1997)]。该模型将这种“软玻璃质材料”流变学的相似性归因于结构无序和亚稳性的共同特征。通过关注介观元素的动力学,它保留了一个通用的字符。相互作用由平均场噪声温度x表示,玻璃化转变发生在x=1(以适当的单位表示)。该模型的精确解采用将应力与应变历史相关联的本构方程的形式,从该本构方程可以导出所有流变性质。对于线性响应,我们发现储能模量G'和损耗模量G“都随频率ω^{x-1}(1<x<2)变化,在玻璃化转变附近变得平坦。在玻璃相,老化的模量预测。稳态剪切流动曲线显示x<2的幂律流体行为,玻璃相中具有非零屈服应力; Cox-Merz规则在该非牛顿状态下不成立。单阶和双阶应变进一步探讨了模型的非线性行为,这是不能很好地表示的BKZ关系。最后,我们考虑在有限应变幅γ下G'和G“的测量。在玻璃化转变附近,随着应变扫描中γ的增加,G“呈现最大值。由于非线性效应,它的值可能会被严重高估,即使当应力响应非常接近谐波时也会出现这种效应。在最大应变γ_c处,测量仍能探测到线性响应,这一点与频率无关。