arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1604.07508cond-mat.mtrl-sci
收藏

不同前驱体浓度条件下金微粒及不同粒径金颗粒的形成

Development of Gold Tiny Particles and Particles in Different Sizes at Varying Precursor Concentration

Mubarak Ali, I-Nan Lin

摘要:

纳米粒子的聚结(或生长)是纳米技术中一个令人兴奋和实用的研究课题。本研究涉及在不同的前体浓度在定制的设置中的金颗粒的发展。在双极脉冲OFF与ON时间的调谐比率下,不同尺寸和形状的微小颗粒取决于金前驱体的量而发展。当金原子在溶液表面形成致密的单分子层组装体时,纳米能量以包的形式将金原子束缚在溶液中。在0.07 mM至0.90 mM前体浓度之间,微小颗粒以三角形和非三角形形状形成。在前体浓度为0.30 mM和0.60 mM时,大量形成三角形的微小颗粒。因此,纳米颗粒和颗粒也以不同的几何形状形成。这种微小的颗粒由于在浸没格式中施加的力而聚集,其中光滑元件的结构组装以形成不同形状的纳米颗粒和颗粒。非几何形状的微小颗粒不会聚集在一个公共点,它们的聚集形成了扭曲或球形的纳米颗粒或颗粒。这主要发生在前体浓度为0.05 mM和1.20 mM时。在50 sccm氩气流速下,纳米颗粒和颗粒以与100 sccm的情况相同的形状形成。对于不同的前体浓度,溶液的不同颜色表示纳米颗粒和颗粒的不同特征。这项研究阐明了必要的浓度的前体开发不同尺寸的胶体。

英文摘要:

Coalescence (or Growth) of tiny particles to larger particles has been an exciting and practical research topic in nanotechnology. This study deals with development of gold particles at varying precursor concentration in a custom-built setup. Under the tuned ratio of bipolar pulse OFF to ON time, tiny particles of different sizes and shapes develop depending on the amount of gold precursor. When compact monolayer assembly is formed on solution surface, nano energy in packet shapes bind gold atoms in own shape. Between 0.07 mM to 0.90 mM precursor concentration, tiny particles develop in both triangular and non-triangular shapes. Tiny particles of triangular shape develop in a large number at precursor concentration 0.30 mM and 0.60 mM. Hence, nanoparticles and particles also developed in different geometrical shapes. Such tiny particles pack due to the exerted force in immersing format, where made structures of smooth elements assemble to develop nanoparticles and particles of different shapes. Tiny particles of non-geometrical shapes do not assemble at a common point and their assembling develops a nanoparticle or particle of distorted or spherical shape. This occurs mainly when precursor concentration is 0.05 mM and 1.20 mM. At 50 sccm Argon flow rate, nanoparticles and particles develop in the same shapes as in case of 100 sccm. For different precursor concentrations, different colors of solutions indicate different features of nanoparticles and particles. This study clarifies the necessary concentration of precursor to develop colloids of different sizes.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑