在金支撑的单层$MoS_{2}$上直接原子层沉积超薄$Al_{2}O_{3}$和$HfO_{2}$薄膜

Direct atomic layer deposition of ultra-thin $Al_{2}O_{3}$ and $HfO_{2}$ films on gold-supported monolayer $MoS_{2}$

E. Schilirò, S. E. Panasci, A. M. Mio, G. Nicotra, S. Agnello, B. Pecz, G. Z. Radnoczi, I. Deretzis, A. La Magna, F. Roccaforte, R. Lo Nigro, F. Giannazzo

AI总结:

本研究通过原子层沉积在金支撑单层MoS2上直接生长超薄Al2O3和HfO2薄膜,揭示了成核机制及高k封装对MoS2应变和光学性质的影响。

摘要:

本文研究了在金支撑的单层(1L)$MoS_{2}$上原子层沉积(ALD)超薄(<4 nm)$Al_{2}O_{3}$和$HfO_{2}$薄膜,从而深入了解ALD过程早期阶段的成核机制。对在溅射生长的Au/Ni薄膜上剥离的大面积1L-$MoS_{2}$进行的初步多尺度表征显示,$MoS_{2}$膜几乎共形地覆盖Au形貌,并在纳米尺度上出现应变变化。$MoS_{2}$/Au(111)界面的从头算DFT计算表明,Au衬底对$MoS_{2}$能带结构有显著影响,而$H_{2}O$、TMA和TDMAHf前驱体的吸附差异较小。这表明纳米尺度的形态效应(如$MoS_{2}$膜的局部曲率和应变)在前驱体的增强物理吸附中起着关键作用。因此,研究了$Al_{2}O_{3}$和$HfO_{2}$薄膜在1L-$MoS_{2}$/Au上的成核和生长,通过监测表面覆盖率随ALD循环次数(N)的变化,N从10到120。在低N值时,观察到$HfO_{2}$初始形成的核生长速率较慢,这可能是由于TDMAHf前驱体与TMA相比体积庞大。另一方面,在N>80个ALD循环时,两种情况均形成了连续薄膜,对应3.6 nm $Al_{2}O_{3}$和3.1 nm $HfO_{2}$。C-AFM的电流映射显示,在相同偏压下,$Al_{2}O_{3}$表现出均匀的绝缘行为,而$HfO_{2}$则出现少量局部击穿点,这与较不致密的薄膜区域有关。最后,用这两种高k薄膜封装后,通过拉曼映射观察到1L-$MoS_{2}$的拉伸应变增加,同时伴随PL强度降低。

英文摘要:

In this paper, the atomic layer deposition (ALD) of ultra-thin films (<4 nm) of $Al_{2}O_{3}$ and $HfO_{2}$ on Au-supported monolayer (1L) $MoS_{2}$ is investigated, providing an insight on the nucleation mechanisms in the early stages of the ALD process. A preliminary multiscale characterization of large area 1L-$MoS_{2}$ exfoliated on sputter-grown Au/Ni films revealed an almost conformal $MoS_{2}$ membrane with the Au topography and the occurrence of strain variations at the nanoscale. Ab-initio DFT calculations of $MoS_{2}$/Au(111) interface showed a significant influence of the Au substrate on the $MoS_{2}$ energy band structure, whereas small differences were accounted for the adsorption of the $H_{2}O$, TMA and TDMAHf precursors. This suggests a crucial role of nanoscale morphological effects, such as local curvature and strain of the $MoS_{2}$ membrane, in the enhanced physisorption of the precursors. Therefore, the nucleation and growth of $Al_{2}O_{3}$ and $HfO_{2}$ films onto 1L-$MoS_{2}$/Au was investigated, by monitoring the surface coverage as a function of the number (N) of ALD cycles, with N from 10 to 120. At low N values, a slower growth rate of the initially formed nuclei was observed for $HfO_{2}$, probably due to the bulky nature of the TDMAHf precursor as compared to TMA. On the other hand, the formation of continuous films was obtained in both cases for N>80 ALD cycles, corresponding to 3.6 nm $Al_{2}O_{3}$ and 3.1 nm $HfO_{2}$. Current mapping by C-AFM showed, for the same applied bias, a uniform insulating behavior of $Al_{2}O_{3}$ and the occurrence of few localized breakdown spots in the case of $HfO_{2}$, associated to less compact films regions. Finally, an increase of the 1L-$MoS_{2}$ tensile strain was observed by Raman mapping after encapsulation with both high-k films, accompanied by a reduction in the PL intensity.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑