Ni-Mn-Ga-Cu铁磁记忆合金逆马氏体相变的巨磁热效应

Giant magnetocaloric effect from reverse martensitic transformation in Ni-Mn-Ga-Cu ferromagnetic shape memory alloys

Sudip Kumar Sarkar, Sarita, P. D. Babu, Aniruddha Biswas, Vasudeva Siruguri, Madangopal krishnan

摘要:

为了在室温附近产生巨磁热效应(GMCE),在首次此类研究中,铁磁记忆合金(FSMA)的奥氏体相变温度(As)被微调到铁磁居里温度(TC),Ni50Mn18.5Cu6.5Ga25合金在逆马氏体相变过程中获得了δ-SM =-81.75 J/Kg-K的大GMCE(加热循环),在302.5 K下磁场变化为9 T。在Ni_(50)Mn_(25-x)Cu_xGa_(25)(0< x < 7.0)基FSMA中通过Cu替代实现了As与TC的微调。这些合金的表征进行了使用光学和扫描电子显微镜,X射线衍射(XRD),差示扫描量热法(DSC)和直流磁化测量。在化学计量比Heusler型Ni_2MnGa中加入Cu可提高马氏体相变温度,降低相变温度。同时,DSM随着Cu的添加而增加,并在6.5at. % Cu,TC和As之间存在虚拟重叠。在302.5K温度下,9 T磁场变化的加热循环中也获得了327.01J/Kg的最大制冷量(RCP)。对于相同的6.5 at.,冷却循环测量的相应值(在正转变期间测量)分别为30.4 J/Kg-K和123.52 J/Kg。% Cu样品和相同的热磁条件。

英文摘要:

In an effort to produce Giant Magnetocaloric effect (GMCE) near room temperature, in a first ever such study, the austenite transformation temperature (As) was fine tuned to ferromagnetic Curie temperature (TC) in Ferromagnetic Shape Memory Alloys (FSMA) and a large GMCE of delta-SM = - 81.75 J/Kg-K was achieved in Ni50Mn18.5Cu6.5Ga25 alloy during reverse martensitic transformation (heating cycle) for a magnetic field change of 9 T at 302.5 K. Fine tuning of As with TC was achieved by Cu substitution in Ni50Mn25-xCuxGa25 (0< x < 7.0)-based FSMAs. Characterizations of these alloys were carried out using Optical and Scanning Electron Microscopy, X-ray Diffraction (XRD), Differential Scanning Calorimetry (DSC) and DC magnetization measurements. Addition of Cu to stoichiometric Heusler type Ni2MnGa increases the martensitic transformation temperatures and decreases TC. Concurrently, DSM increases with Cu addition and peaks at 6.5 at. % Cu for which there is a virtual overlap between TC and As. Maximum Refrigerant Capacity (RCP) of 327.01 J/Kg was also achieved in the heating cycle for 9 T field change at 302.5 K. Corresponding values for the cooling cycle measurements (measured during forward transformation) were 30.4 J/Kg-K and 123.52 J/Kg respectively for the same 6.5 at. % Cu sample and same thermo-magnetic conditions.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑