arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1301.4069cond-mat.mtrl-scicond-mat.str-el
收藏

尺寸失配引起的淬火无序对多晶$Nd_{0.58-x} Gd_x Sr_{0.42} Mn O_3$相位涨落和低场磁输运的影响

Impact of size mismatch induced quenched disorder on phase fluctuation and low field magnetotransport in polycrystalline $Nd_{0.58-x} Gd_x Sr_{0.42} Mn O_3$

Manoj K. Srivastava, Ravikant Prasad, P. K. Siwach, M. P. Singh, H. K. Singh

摘要:

本文报道了在1350 ℃下用固相反应法合成的大块多晶NGSMO(x ~ 0.0,0.04,0.08,0.12,0.16,0.20,0.25,0.30,0.35和0.42)的磁和电输运性质。所有样品均为单相,晶粒尺寸约为1-2微米。磁性和磁输运性质随方差σ ^[2]的变化呈现出一些有趣的趋势。随着σ ^[2]的增加,顺磁-铁磁(PM-FM)转变逐渐减小并变宽,而绝缘体-金属转变(IMT)的减小伴随着尖锐化。然而,在σ 2的中间值处的TC和TIM的接近相等可以理解为竞争淬火和晶界无序。峰值MR(TC/TIM附近的最大MR)随σ 2的变化表明,H=3 kOe时的最大低场MR = 35%(H=10 kOe时为68%)集中在σ 2 = 0.009857 {A}2(x=0.25)附近。这表明,在相位起伏增强的区域,在相对较高的温度和较低的磁场下可以获得巨大的本征MR。

英文摘要:

We report the magnetic and electrical transport properties of the bulk polycrystalline NGSMO (x ~ 0.0, 0.04, 0.08, 0.12, 0.16, 0.20, 0.25, 0.30, 0.35 and 0.42) synthesized by solid state reaction at 1350 degree Celsius. All the samples are single phase and have grain size ~1-2 micrometer. The variation of magnetic and magnetotransport properties as a function of the variance sigma^2 show some interesting trends. As sigma^2 increases, the paramagnetic-ferromagnetic (PM-FM) transition shows a gradual decrease and broadening, while the decrease in insulator metal transition (IMT) is accompanied by sharpening. However, near equality of TC and TIM at intermediate values of sigma2 could be understood in terms of the competing quenched and the grain boundary disorder. The variation of peak MR (maximum MR around TC/TIM) with sigma2 shows that maximum low field MR =35 % at H=3 kOe (68 % at H=10 kOe) is centered around sigma2 = 0.009857 {A}2 (x=0.25). This shows that huge intrinsic MR can be obtained at relatively higher temperatures and lower magnetic fields in the region of enhanced phase fluctuations.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑