arXiv 1212.4829cond-mat.mtrl-sci
收藏

研究了混合价钴酸盐Nd $_{0.7}$ Sr PDMATHAAB CoO PDMATHAAD、Nd $_{0.7}$ Ca PDMATHAAB CoO PDMATHAAD和Pr $_{0.7}$ Ca $_{0.3}$ PDKEEPAAAD $_3$的基态性质

The ground state properties of the mixed-valence cobaltites Nd$_{0.7}$Sr$_{0.3}$CoO$_3$, Nd$_{0.7}$Ca$_{0.3}$CoO$_3$ and Pr$_{0.7}$Ca$_{0.3}$CoO$_3$

Z. Jirak, J. Hejtmanek, K. Knizek, M. Marysko, P. Novak, E. Santava, T. Naito, H. Fujishiro

摘要:

研究了三种具有相同30%空穴掺杂和铁磁基态的钙钛矿型钴酸盐的电、磁和热性质,直到很低的温度。随着大阳离子尺寸的减小,钴的铁磁居里温度和自发磁矩逐渐被抑制-对于Nd $_{0.7}$ Sr $_{0.3}$ CoO $_3$、Pr $_{0.7}$ Ca $_{0.3}$ CoO $_3$和Nd $_{0.7}$ Ca $_{0.3}$ CoO $_3$,分别为$T_C=130$ K,55 K和25 K以及$m = 0.68 μ_B$,0.34 $μ_B$和0.23 $μ_B$。对于Co $^{3+}$ /Co $^{4+}$,相对于传统铁磁体La $_{0.7}$ Sr $_{0.3}$ CoO $_3$($T_C=230$ K,$m = 1.71 μ_B$)在所谓IS/LS状态下的磁矩的磁矩减少最初使用相分离方案来解释。基于目前的结果,主要是肖特基峰的分析起源于塞曼分裂的基态Kramers双峰的Nd $^{3+}$,我们发现,然而,在Nd $_{0.7}$ Ca $_{0.3}$ CoO $_3$和可能也Pr $_{0.7}$ Ca $_{0.3}$ CoO $_3$的铁磁相是均匀分布在所有的样品体积,尽管严重下降的时刻。这些化合物的基态由Sboychakov \textit{et al.} [Phys. Rev. \textbf{80},024423(2009)]理论上推导的LS/LS相关相确定。由于LS/LS和IS/LS相的竞争,具有中等钴矩的Nd $_{0.7}$ Sr $_{0.3}$ CoO $_3$的基态是不均匀的。在理论研究部分,计算了$4f^3$(Nd $^{3+}$)、$4f^2$(Pr $^{3+}$)和$4f^1$(Ce $^{3+}$或Pr $^{4+}$)的晶场分裂能级,并给出了它们的磁特性。

英文摘要:

The electric, magnetic, and thermal properties of three perovskite cobaltites with the same 30% hole doping and ferromagnetic ground state were investigated down to very low temperatures. With decreasing size of large cations, the ferromagnetic Curie temperature and spontaneous moments of cobalt are gradually suppressed - $T_C=130$ K, 55 K and 25 K and $m = 0.68 μ_B$, 0.34 $μ_B$ and 0.23 $μ_B$ for Nd$_{0.7}$Sr$_{0.3}$CoO$_3$, Pr$_{0.7}$Ca$_{0.3}$CoO$_3$ and Nd$_{0.7}$Ca$_{0.3}$CoO$_3$, respectively. The moment reduction with respect to moment of the conventional ferromagnet La$_{0.7}$Sr$_{0.3}$CoO$_3$ ($T_C=230$ K, $m = 1.71 μ_B$) in so-called IS/LS state for Co$^{3+}$/Co$^{4+}$, was originally interpreted using phase-separation scenario. Based on the present results, mainly the analysis of Schottky peak originating in Zeeman splitting of the ground state Kramers doublet of Nd$^{3+}$, we find, however, that ferromagnetic phase in Nd$_{0.7}$Ca$_{0.3}$CoO$_3$ and likely also Pr$_{0.7}$Ca$_{0.3}$CoO$_3$ is uniformly distributed over all sample volume, despite the severe drop of moments. The ground state of these compounds is identified with the LS/LS-related phase derived theoretically by Sboychakov \textit{et al.} [Phys. Rev. B \textbf{80}, 024423 (2009)]. The ground state of Nd$_{0.7}$Sr$_{0.3}$CoO$_3$ with an intermediate cobalt moment is inhomogeneous due to competing of LS/LS and IS/LS phases. In the theoretical part of the study, the crystal field split levels for $4f^3$ (Nd$^{3+}$), $4f^2$ (Pr$^{3+}$) and $4f^1$ (Ce$^{3+}$ or Pr$^{4+}$) are calculated and their magnetic characteristics are presented.