MOD derived pyrochlore films as buffer layer for all-chemical YBCO coated conductors

Andrea Augieri, Angelo Vannozzi, Rita Mancini, Achille Armenio Angrisani, Fabio Fabbri, Valentina Galluzzi, Alessandro Rufoloni, Francesco Rizzo, Antonella Manc… 展开作者

Andrea Augieri, Angelo Vannozzi, Rita Mancini, Achille Armenio Angrisani, Fabio Fabbri, Valentina Galluzzi, Alessandro Rufoloni, Francesco Rizzo, Antonella Mancini, Giuseppe Celentano, Ivan Colantoni, Ivan Davoli, Nicola Pompeo, Giovanni Sotgiu, Enrico Silva

摘要:

本文报道了用金属有机物分解法(MOD)生长的La_2Zr_2O_7(LZO)烧绿石材料作为YBa_2Cu_3O_(7-x)(YBCO)涂层导体的缓冲层的详细研究。在单晶和Ni-5%at.W衬底上获得了高质量的LZO薄膜。为了评估薄膜的结构和形态特性,通过X射线衍射分析(XRD)、原子力显微镜(AFM)和扫描电子显微镜(SEM)对薄膜进行了表征。通过热重分析(TG-DTA-DTG)和红外光谱(FT-IR)对前驱体溶液和热处理进行了研究,旨在优化退火工艺。在此缓冲层上用脉冲激光烧蚀法(PLD)沉积了YBCO薄膜。在SC上获得的最佳结果表明,YBCO薄膜的临界温度值高于90 K,在77 K下具有高的自场临界电流密度(Jc > 1 MA/cm 2)和高的不可逆场(8.3 T),微波下测得的脱钉频率vp(0.5 T,77 K)>44 GHz。在Ni-5%at.W上已经获得了最好的结果,在热处理中在空气中在低温下引入热解过程以除去前体溶液的残留有机部分。

英文摘要:

We report a detailed study performed on La2Zr2O7 (LZO) pyrochlore material grown by Metal-Organic Decomposition (MOD) method as buffer layers for YBa2Cu3O7-x (YBCO) coated conductors. High quality epitaxial LZO thin films have been obtained on single crystal (SC) and Ni-5%at.W substrates. In order to evaluate structural and morphological properties, films have been characterized by means of X-ray diffraction analyses (XRD), atomic force microscope (AFM) and scanning electron microscope (SEM). Precursors solutions and heat treatments have been studied by thermogravimetric analyses (TG-DTA-DTG) and infrared spectra (FT-IR) with the aim of optimizing the annealing process. Thin films of YBCO have been deposited by pulsed laser ablation (PLD) on this buffer layers. The best results obtained on SC showed YBCO films with critical temperature values above 90 K, high self field critical current density values (Jc > 1 MA/cm2) and high irreversibility field values (8.3 T) at 77 K together with a rather high depinning frequency vp (0.5 T, 77 K)>44 GHz as determined at microwaves. The best results on Ni-5%at.W has been obtained introducing in the heat treatment a pyrolysis process at low temperature in air in order to remove the residual organic part of the precursor solution.