超声喷雾热解法制备掺铥和掺镱氧化钛薄膜
Thulium and ytterbium-doped titanium oxide thin films deposited by ultrasonic spray pyrolysis
摘要:
采用金属有机喷雾热分解沉积法,以二乙酰丙酮钛(IV)、三乙酰丙酮铥(III)和三乙酰丙酮镱(III)为原料,制备了掺铥和掺镱的二氧化钛薄膜。研究了300°C至600°C的沉积温度。薄膜的结晶度和掺杂质量进行了研究。用电子探针、X射线衍射和傅里叶变换红外光谱对TiO 2:Tm,Yb的结构和组成进行了表征。沉积速率可达0.8 \mum /h。在400°C或更高温度下合成后获得TiO 2的锐钛矿相。在低沉积温度下,通过退火处理消除有机污染。
英文摘要:
Thin films of thulium and ytterbium-doped titanium oxide were grown by metal-organic spray pyrolysis deposition from titanium(IV)oxide bis(acetylacetonate), thulium(III) tris(2,2,6,6-tetramethyl-3,5-heptanedionate) and ytterbium(III) tris(acetylacetonate). Deposition temperatures have been investigated from 300°C to 600°C. Films have been studied regarding their crystallity and doping quality. Structural and composition characterisations of TiO2:Tm,Yb were performed by electron microprobe, X-ray diffraction and Fourier transform infrared spectroscopy. The deposition rate can reach 0.8 \mum/h. The anatase phase of TiO2 was obtained after synthesis at 400°C or higher. Organic contamination at low deposition temperature is eliminated by annealing treatments.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。