MOCVD沉积铥镱掺杂二氧化钛薄膜
Thulium and ytterbium-doped titania thin films deposited by MOCVD
摘要:
在这项研究中,我们合成的薄膜的二氧化钛掺杂铥和/或镱修改的入射光谱的太阳能电池。这可以通过光致发光上转换装置或下转换装置来实现。作为降频转换薄膜,我们的工作涉及到铥和镱掺杂的钛白。铥和镱将分别充当敏化剂和发射体。稀土掺杂薄膜是通过气溶胶辅助MOCVD使用有机金属前体,如溶解在不同溶剂中的钛白乙酰丙酮化物、铥和四甲基庚二酸镱沉积的。这些薄膜已经在不同的沉积条件(例如温度和掺杂剂浓度)下沉积在硅衬底上。已经在300°C至600°C的沉积温度范围内获得了粘附膜。沉积速率为0.1 ~ 1 μm/h。在高于400°C的衬底温度下获得α相。需要进一步退火以显示发光并消除前体的有机残余物。分析了不同沉积参数和退火条件下薄膜的物理化学和发光特性。我们发现,在近紫外线蓝色范围内的吸收光被重新发射的镱在980 nm,并通过一个thuralite带约800 nm。
英文摘要:
In this study we synthesized thin films of titanium oxide doped with thulium and/or ytterbium to modify the incident spectrum on the solar cells. This could be achieved either by photoluminescence up-converting devices, or down-converting devices. As down-converter thin films our work deals with thulium and ytterbium-doped titanium dioxide. Thulium and ytterbium will act as sensitizer and emitter, respectively. The rare-earth doped thin films are deposited by aerosol-assisted MOCVD using organo-metallic precursors such as titanium dioxide acetylacetonate, thulium and ytterbium tetramethylheptanedionate solved in different solvents. These films have been deposited on silicon substrates under different deposition conditions (temperature and dopant concentrations for example). Adherent films have been obtained for deposition temperatures ranging from 300°C to 600°C. The deposition rate varies from 0.1 to 1 μm/h. The anatase phase is obtained at substrate temperature above 400°C. Further annealing is required to exhibit luminescence and eliminate organic remnants of the precursors. The physicochemical and luminescent properties of the deposited films were analyzed versus the different deposition parameters and annealing conditions. We showed that absorbed light in the near-UV blue range is re-emitted by the ytterbium at 980 nm and by a thulium band around 800 nm.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。