(La0)0.7Pb0.3MnO3单晶在脉冲磁场下的磁电阻弛豫

Magnetoresistance Relaxation in (La0.5Eu0.5)0.7Pb0.3MnO3 Single Crystals under the Action of a Pulse Magnetic Field

A. A. Bykov, S. I. Popkov, K. A. Shaykhutdinov, K. A. Sablina

摘要:

在脉冲磁场H = 25 T下,测量了不同温度下掺杂镧锰氧化物(La 0.5Eu 0.5)0.7Pb 0.3MnO 3的磁电阻。发现了特征时间为10 - 3s的磁电阻弛豫,并确定了弛豫参数τ(t)随温度的变化与电阻R(T)随温度的变化关系。建议的松弛机制是有关的相分层条件下的样品体积中的导电和介电相的松弛。结果表明,弛豫参数τ反映的是体积中的边界数,而不是相分数的比值。

英文摘要:

Magnetoresistance of substituted lanthanum manganite (La0.5Eu0.5)0.7Pb0.3MnO3 in the pulse magnetic field H = 25 T was measured at different temperatures. Magnetoresistance relaxation with a characteristic time of 10 -3 s was found. It has been established that the temperature dependence of the relaxation parameter τ(t) at different temperatures correlates with the temperature dependence of electrical resistance R(T). The proposed relaxation mechanism is related to relaxation of conducting and dielectric phases in the sample volume under phase stratification conditions. It is shown that relaxation parameter τ reflects the number of boundaries in the volume and not the ratio between phase fractions.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑