自燃烧法合成Cu[x]Co[1-x] Fe2O4纳米结构的磁性和湿敏特性
Magnetic and humidity sensing properties of nanostructured Cu[x]Co[1-x]Fe2O4 synthesized by auto combustion technique
摘要:
采用自燃烧法合成了Cu-$_x$-Co $_{1-x}$-Fe $_2$ O $_4$-(x = 0.0,0.5和1.0)磁性纳米材料(23-43 nm)。这些材料的微晶尺寸由X射线衍射峰计算。在这些样品中在575 cm $^{-1}$附近的傅里叶变换红外光谱中观察到的谱带证实了铁氧体相的存在。电导率测量显示了热滞后,并证明了对于铜铁氧体、钴铁氧体和铜-钴混合铁氧体,分别在475 $^o$ C、525 $^o$ C和500 $^o$ C处的拐点。使用振动样品磁强计(VSM)跟踪这些材料的磁滞M-H环,并且表明由于Cu $^{2+}$离子在钴铁氧体中的取代,饱和磁化强度(M $_s$)和剩磁(M $_r$)显著增加,而本征矫顽力(H $_c$)降低。在这些铁氧体中,铜铁氧体对湿度的敏感性最高。
英文摘要:
Magnetic nanomaterials (23-43 nm) of Cu$_x$Co$_{1-x}$Fe$_2$O$_4$\ (x = 0.0, 0.5 and 1.0) were synthesized by auto combustion method. The crystallite sizes of these materials were calculated from X-ray diffraction peaks. The band observed in Fourier transform infrared spectrum near 575 cm$^{-1}$ in these samples confirm the presence of ferrite phase. Conductivity measurement shows the thermal hysteresis and demonstrates the knee points at 475$^o$C, 525$^o$C and 500$^o$C for copper ferrite, cobalt ferrite and copper-cobalt mixed ferrite respectively. The hystersis M-H loops for these materials were traced using the Vibrating Sample Magnetometer (VSM) and indicate a significant increase in the saturation magnetization (M$_s$) and remanence (M$_r$) due to the substitution of Cu$^{2+}$ ions in cobalt ferrite, while the intrinsic coercivity (H$_c$) was decreasing. Among these ferrites, copper ferrite exhibits highest sensitivity for humidity.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。