Analysis of strain and stacking faults in single nanowires using Bragg coherent diffraction imaging
V. Favre-Nicolin, F. Mastropietro, J. Eymery, D. Camacho, Y. M. Niquet, B. M. Borg, M. E. Messing, L. -E. Wernersson, R. E. Algra, E. P. A. M. Bakkers, T. H. Me… 展开作者
V. Favre-Nicolin, F. Mastropietro, J. Eymery, D. Camacho, Y. M. Niquet, B. M. Borg, M. E. Messing, L. -E. Wernersson, R. E. Algra, E. P. A. M. Bakkers, T. H. Metzger, R Harder, I. K. Robinson
备注:
18 pages, 6 figures Submitted to New Journal of Physics
Coherent diffraction imaging (CDI) on Bragg reflections is a promising technique for the study of three-dimensional (3D) composition and strain fields in nanostructures, which can be recovered directly from the coherent diffraction data recorded on single objects. In this article we report results obtained for single homogeneous and heterogeneous nanowires with a diameter smaller than 100 nm, for which we used CDI to retrieve information about deformation and faults existing in these wires. The article also discusses the influence of stacking faults, which can create artefacts during the reconstruction of the nanowire shape and deformation.
A Surface Stacking Fault Energy Approach to Predicting Defect Nucleation in Surface-Dominated Nanostructures
我们提出了一个表面堆垛层错(SSF)能量的方法来预测缺陷成核从表面占主导地位的纳米结构,如FCC金属纳米线的表面。该方法导致一个标准,预测初始屈服机制,通过滑移或孪晶取决于是否不稳定的孪晶能量或不稳定的滑移能量是从所得SSF能量曲线确定的较小。该方法通过SSF能量计算和低温经典分子动力学模拟之间的比较与不同的轴向和横向表面取向,和横截面的几何形状的铜纳米线进行验证。我们专注于几何截面的影响,通过研究从滑移到孪晶的过渡先前预测的移动从正方形到矩形截面的$\ <100\ > /\{100\}$纳米线,也为移动从菱形到截断菱形截面几何形状的$\ <110\ >$纳米线。\hsp{We also provide the important demonstration that the criteria is able to predict the correct deformation mechanism when full dislocation slip is considered concurrently with partial dislocation slip and twinning. This is done in the context of rhombic aluminum nanowires which do not show a tensile reorientati…
Beam damage of single semiconductor nanowires during X-ray nano beam diffraction experiments
纳米探针X射线衍射(nXRD)是一种利用聚焦同步辐射来研究单个半导体纳米线结构特性的强有力的技术。然而,当在环境条件下进行实验时,所需的高X射线剂量和延长的暴露时间可导致辐射损伤。为了揭示辐射损伤的起源,我们比较了在第三代源PETRA III的P08光束线的微焦点站在环境条件下和在He气氛下对单个半导体纳米线的生长几何形状进行的nXRD实验。使用9 keV的入射X射线束能量和10 $^{10}$ s $^{-1}$的光子通量,通过在几个小时内连续记录在固定空间位置处的111布拉格反射的倒易空间图来监测单个GaAs/In $_{0.2}$ Ga $_{0.8}$ As/GaAs核-壳纳米线的轴向晶格参数和倾斜。此外,(In,Ga)As量子阱的发射特性,暴露的纳米线的原子组成和纳米线的形态进行了研究,分别通过阴极发光光谱,能量色散X射线光谱和扫描电子显微镜,无论是之前和之后的nXRD曝光。暴露在环境条件下的纳米线显示出严重的光学和形态学损伤,这是减少暴露在He气氛下的纳米线。所观察到的损伤可以在很大程度上归因于空气中X射线引起的臭氧反应的氧化过程。由于与GaAs相比较低的传热系数,该氧化物壳限制了通过纳米线侧刻面的传热,这被认为是生长几何形状中纳米线散热的主要通道。
Spatially-resolved luminescence and crystal structure of single core-shell nanowires measured in the as-grown geometry
我们报道了单个的、生长态的核-多壳GaAs/In $_{0.15}$ Ga $_{0.85}$ As/GaAs/AlAs/GaAs纳米线的结构和光学性质之间的直接相关性。通过分子束外延在预先图案化的Si(111)衬底上制造,在一排良好分离的成核位置上,可以在生长的几何形状中访问单个纳米线。通过同步辐射纳米探针X射线衍射技术监测轴向111布拉格反射,揭示了沿纳米线生长轴的多型体分布。对于相同的纳米线,空间分辨的发射特性,通过阴极发光高光谱线扫描在扫描电子显微镜。相关的两个测量,我们揭示了一个蓝移的壳量子阱发射能量结合的发射强度增加的片段表现出的混合结构的交替纤锌矿和锌的堆叠相比,纯晶体多型体。这种混合结构的存在下,独立地证实了横截面透射电子显微镜。