陶瓷坯体微压纹力学响应的研究

Study of mechanical response in embossing of ceramic green substrate by micro-indentation

Y. C. Liu, X. -C. Shan

摘要:

采用平头圆锥微压入试验模拟了陶瓷基片的微压印过程,研究了陶瓷基片的热-力响应。以低温共烧陶瓷坯带为试验材料,研究了25 ℃和75 ℃两种温度下压入深度与外加力和外加应力的关系。结果表明,在25 ° C至75 ° C的温度范围内可以形成永久性压痕腔,并且所产生的腔的深度取决于所施加的力、温度和停留时间。蠕变发生,并作出了较大的贡献,在高温和高峰值载荷下的塑性变形。卸载过程中出现瞬时回复,压痕后第一天出现延迟回复。由于在高达75 ℃的温度下压缩时观察到的材料流动,没有明显的堆积。塑性变形是陶瓷坯体在压缩过程中产生空洞的主要原因。研究结果可作为陶瓷坯体模压成型的指导依据。

英文摘要:

Micro-indentation test with a micro flat-end cone indenter was employed to simulate micro embossing process and investigate the thermo-mechanical response of ceramic green substrates. The laminated low temperature co-fired ceramic green tapes were used as the testing material ; the correlations of indentation depth versus applied force and applied stress at the temperatures of 25 degrees C and 75degrees C were studied. The results showed that permanent indentation cavities could be formed at temperatures ranging from 25 degrees C to 75 degrees C, and the depth of cavities created was applied force, temperature and dwell time dependent. Creep occurred and made a larger contribution to the plastic deformation at elevated temperatures and high peak loads. There was instantaneous recovery during the unloading and retarded recovery in the first day after indentation. There was no significant pile-up due to material flow observed under compression at the temperature up to 75 degrees C. The plastic deformation was the main cause for formation of cavity on the ceramic green substrate under compression. The results can be used as a guideline for embossing ceramic green substrates.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑