热压成形中聚合物变形与回复的研究
Studies of Polymer Deformation and Recovery in Hot Embossing
摘要:
在大面积微热压成形中,工艺温度对微结构成形的局部保真度和整体均匀性都起着至关重要的作用。低温热压的意义在于提高压纹器件的整体平整度。本文报道了在微压印过程中,当工艺温度低于或接近聚合物的玻璃化转变温度(Tg)时,聚合物的变形和松弛的实验研究。在这项研究中,压痕系统和显微硬度计被用来研究微结构的形成与工艺温度和负载压力的关系。控制压入深度,测量一定压入深度下的载荷。使用1 mm厚的PMMA膜进行实验,加工温度范围为Tg-55 ℃至Tg +20 ℃。压印结构包括单个微腔和多组微腔阵列。结果表明,在Tg-55 ℃温度下,微结构的形成以弹性变形为主,压印后微结构发生明显的松弛。从Tg-20 ℃到Tg,塑性变形占主导地位的聚合物变形,并可以在PMMA基板上形成永久性空腔没有明显的弛豫。然而,作为微柱的膨胀结构的形成是不完全的,因为几乎没有聚合物流动。随着加工温度的升高,在较低的加载压力下即可形成微结构。考虑到单个微结构的保真度和压花基材的整体平坦度,应优选在低工艺温度下但具有良好保真度的微热压花。
英文摘要:
In large area micro hot embossing, the process temperature plays a critical role to both the local fidelity of microstructure formation and global uniformity. The significance of low temperature hot embossing is to improve global flatness of embossed devices. This paper reports on experimental studies of polymer deformation and relaxation in micro embossing when the process temperatures are below or near its glass transition temperature (Tg). In this investigation, an indentation system and a micro embosser were used to investigate the relationship of microstructure formation versus process temperature and load pressure. The depth of indentation was controlled and the load force at a certain indentation depth was measured. Experiments were carried out using 1 mm thick PMMA films with the process temperature ranging from Tg-55 degrees C to Tg +20 degrees C. The embossed structures included a single micro cavity and groups of micro cavity arrays. It was found that at temperature of Tg-55 degrees C, elastic deformation dominated the formation of microstructures and significant relaxation happened after embossing. From Tg-20 degrees C to Tg, plastic deformation dominated polymer deformation, and permanent cavities could be formed on PMMA substrates without obvious relaxation. However, the formation of protrusive structures as micro pillars was not complete since there was little polymer flow. With an increase in process temperature, microstructure could be formed under lower loading pressure. Considering the fidelity of a single microstructure and global flatness of embossed substrates, micro hot embossing at a low process temperature, but with good fidelity, should be preferred.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。