arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 0805.0504cond-mat.mes-hall
收藏

Ga0.25 In 0.75 As量子点接触中增强的塞曼分裂

Enhanced Zeeman splitting in Ga0.25In0.75As quantum point contacts

T. P. Martin, A. Szorkovszky, A. P. Micolich, A. R. Hamilton, C. A. Marlow, H. Linke, R. P. Taylor, L. Samuelson

摘要:

外加磁场诱导的塞曼分裂强度是介观器件实现自旋分辨输运的重要因素。我们测量的塞曼分裂的量子点接触蚀刻到Ga 0.25In 0.75As量子阱,与场取向平行于输运方向。我们观察到Lande g因子的增强,|g*|=3.8 +/- 0.2,对于第三子带,|g*|=5.8 +/- 0.6,比GaAs大六倍。我们报告的子带间距超过10毫电子伏,这有利于在更高的温度下的量子输运。

英文摘要:

The strength of the Zeeman splitting induced by an applied magnetic field is an important factor for the realization of spin-resolved transport in mesoscopic devices. We measure the Zeeman splitting for a quantum point contact etched into a Ga0.25In0.75As quantum well, with the field oriented parallel to the transport direction. We observe an enhancement of the Lande g-factor from |g*|=3.8 +/- 0.2 for the third subband to |g*|=5.8 +/- 0.6 for the first subband, six times larger than in GaAs. We report subband spacings in excess of 10 meV, which facilitates quantum transport at higher temperatures.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑