LixCoO2和NaxCoO2体系x = 0端元CoO2的合成与性质
Synthesis and properties of CoO2, the x = 0 end member of the LixCoO2 and NaxCoO2 systems
摘要:
在这里,我们报告的合成单相散装样品的CoO2,x = 0的AxCoO2系统(A = Li,Na),从一个原始的LiCoO2样品,使用电化学技术完全脱嵌锂的末端成员。因此,合成的CoO2样品被发现是氧化学计量的,并具有由堆叠的三角晶格CoO2层的晶体结构。的CoO2样品的磁化率被发现是相对较大的,在其初始值,然后随着温度的升高,这表明CoO2是一个保利顺磁金属与巡回电子。
英文摘要:
We report here the synthesis of single-phase bulk samples of CoO2, the x = 0 end member of the AxCoO2 systems (A = Li, Na), from a pristine LiCoO2 sample using an electrochemical technique to completely de-intercalate lithium. Thus, synthesized CoO2 samples were found to be oxygen-stoichiometric and possess a crystal structure consisting of stacked triangular-lattice CoO2 layers only. The magnetic susceptibility of the CoO2 sample was revealed to be relatively large in its initial value and then level off as the temperature increases, suggesting that CoO2 is a Pauli-paramagnetic metal with itinerant electrons.