arXivDaily arXiv每日学术速递 周一至周五更新
arXiv周末暂无论文更新,休息一下吧,周末愉快~~
arXiv physics/0306125physics.chem-ph
收藏

自增湿Polymer电解质膜燃料电池

The Autohumidification Polymer Electrolyte Membrane Fuel Cell

J. B. Benziger, J. Moxley, S. Tulyani, A. Turner, A. B. Bocarsly, Y. G. Kevrekidis

摘要:

一个PEM燃料电池是专门建造的,以确定在良好定义的气相组成和电池温度的条件下的动力学。在自增湿PEM燃料电池中发现了稳态多重性,这是由水产生和水去除之间的平衡引起的。在PEM燃料电池中观察到点火,临界水活度约为0.1。点火是质子传导率随水活度呈指数增加的结果,这在水的产生和质子传导之间产生自催化反馈。点燃状态下的稳态电流随着温度在50至105摄氏度之间的升高而降低。在高于70摄氏度的温度下,在PEM燃料电池中观察到五个稳态。稳态性能已经遵循可变负载电阻和磁滞回线已被映射。稳态之间的动态转换大约慢10^3到10^4秒。这些缓慢的动力学被认为是由膜电极组件的机械和化学性质的耦合导致的,由于膜的溶胀与水的吸收。

英文摘要:

A PEM fuel cell was specially constructed to determine kinetics under conditions of well-defined gas phase composition and cell temperature. Steady state multiplicity was discovered in the autohumidification PEM fuel cell, resulting from a balance between water production and water removal. Ignition was observed in the PEM fuel cell for a critical water activity of about 0.1. Ignition is a consequence of the exponential increase of proton conductivity with water activity, which creates an autocatalytic feedback between the water production and the proton conduction. The steady state current in the ignited state decreases with increasing temperature between 50 to 105 deg C. At temperatures greater than 70 deg C five steady states were observed in the PEM fuel cell. The steady state performance has been followed with variable load resistance and hysteresis loops have been mapped. The dynamics of transitions between steady states are slow about 10^3 to 10^4 s. These slow dynamics are suggested to result from a coupling of mechanical and chemical properties of the membrane electrode assembly due to swelling of the membrane with water absorption.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑