具有(101)取向微晶的厚MgB2膜

Thick MgB2 film with (101) oriented micro-crystals

Chinping Chen, Xinfeng Wang, Ying Lu, Zhang Jia, Jing-pu Guo, Xiao-nan Wang, Meng Zhu, Xiangyu Xu, Jun Xu, Qing-rong Feng

摘要:

非常厚的,~ 40 $μ$ m,干净,和高度织构的MgB 2薄膜有效地生长在Al 2 O 3衬底上。制备技术是通过混合物理化学气相沉积(HPCVD),使用B2 H6气体和Mg锭作为源。X射线衍射(XRD)分析显示出高度(101)取向的MgB 2晶体结构,没有检测到任何杂质。在XRD光谱中没有来自衬底的信号,表明膜厚度超过X射线穿透长度。扫描电子显微镜(SEM)显示该膜由高度堆积的MgB 2微晶组成,其具有直径约2 $μ$ m和厚度约0.2 $μ$ m的均匀尺寸分布。根据能量色散X射线光谱(EDX)的组成分析,在织构化膜中不存在氧,因此不存在MgO,这与XRD结果一致。此外,传输特性类似于单晶的那些,表明良好微晶的干净膜。零场转变温度确定为TC(开始)= 39.2 K和TC(零)= 38.4 K,给出了干净样品典型的急剧转变。在40 K、9 T的磁场下测得其剩余电阻率比(RRR)为6.4,磁阻(MR)为28%,与单晶的结果相近。零温上临界场HC 2(0)由施加场至9 T时的TC(起始)外推为19 T。

英文摘要:

Very thick, ~ 40 $μ$m, clean, and highly textured MgB2 film was effectively grown on an Al2O3 substrate. The fabrication technique is by the hybrid physical-chemical vapor deposition (HPCVD) using B2H6 gas and Mg ingot as the sources. The X-ray diffraction (XRD) analysis shows a highly (101)-oriented MgB2 crystal structure without any impurity detected. There is no signal from the substrate in the XRD spectrum, indicating that the film thickness exceeds the X-ray penetration length. Scanning electron microscopy (SEM) reveals that the film is composed of highly-packed MgB2 micro-crystals with a uniform size distribution of about 2 $μ$m in diameter and 0.2 $μ$m in thickness. According to the compositional analysis of energy-dispersive X-ray spectroscopy (EDX), no oxygen, hence no MgO, exists in the textured film, consistent with the XRD result. Also, the transport properties are similar to those of a single crystal, indicating a clean film of good crystallite. The zero field transition temperatures are determined as TC(onset) = 39.2 K and TC(zero) = 38.4 K, giving a sharp transition typical of a clean sample. The residual resistivity ratio (RRR) is determined as 6.4 and the magnetoreisitance (MR) is about 28 % at 40 K under the applied field of 9 T, which are similar to those of a single crystal. The zero temperature upper critical field, HC2(0), is extrapolated as 19 T from the TC(onset) at applied field up to 9 T.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑