过冷液态钯的结晶动力学
Crystallisation kinetics of supercooled liquid palladium
AI总结:
采用经典分子动力学模拟研究过冷液态钯的结晶动力学,通过分析微观结构演化确定成核与生长速率,构建时间-温度-转变图,并与快速淬火Pd薄膜的时间分辨X射线衍射实验对比,表明均匀成核主导实验中的过冷度。
摘要:
在本研究中,我们采用经典分子动力学(MD)模拟研究过冷液态钯的结晶动力学,并将结果与快速淬火Pd薄膜的时间分辨X射线衍射测量相关联。通过分析液-晶转变过程中微观结构的演化,确定了温度范围$700$--$1150~\mathrm{K}$($0.38$--$0.65 T_{\mathrm{m}}$)内的晶核形成和生长速率。由原子均方位移得到的Pd自扩散系数在所研究的温度范围内遵循阿伦尼乌斯行为,活化能为$467(6)~\mathrm{meV/atom}$,与过冷液态金属的现有数据一致。稳态均匀成核速率在$0.5 T_{\mathrm{m}}$附近达到最大值约$4 imes 10^{35}~\mathrm{m^{-3} s^{-1}}$。晶体生长速度约为每秒米量级,其温度依赖性符合扩散限制的Wilson-Frenkel动力学,而非碰撞限制机制。基于多个统计独立的模拟,构建了结晶起始的时间-温度-转变(TTT)图。TTT曲线在$0.5 T_{\mathrm{m}}$和$100~\mathrm{ps}$附近出现鼻点,对应的玻璃化临界冷却速率约为$10^{13}~\mathrm{K s^{-1}}$。模拟结果再现了以$5 imes 10^{11}~\mathrm{K s^{-1}}$淬火的光学熔化Pd薄膜的时间分辨X射线衍射实验中观察到的结晶起始时间和温度。这些结果表明,在所研究的实验薄膜中,均匀成核而非非均匀成核主导了可实现的过冷度。
英文摘要:
In this study, we employ classical molecular dynamics (MD) simulations to investigate the crystallisation kinetics of supercooled liquid palladium and relate the results to time-resolved X-ray diffraction measurements on rapidly quenched Pd thin films. Crystal nucleation and growth rates are determined over the temperature range $700$--$1150~\mathrm{K}$ ($0.38$--$0.65 T_{\mathrm{m}}$) by analysing the evolution of the microstructure during the liquid-to-crystal transition. The self-diffusion coefficient of Pd, obtained from the atomic mean-squared displacement, follows Arrhenius behaviour over the investigated temperature range, with an activation energy of $467(6)~\mathrm{meV/atom}$, consistent with available data for supercooled liquid metals. The steady-state homogeneous nucleation rate exhibits a maximum of approximately $4 \times 10^{35}~\mathrm{m^{-3} s^{-1}}$ near $0.5 T_{\mathrm{m}}$. Crystal growth occurs at velocities of the order of metres per second, with a temperature dependence consistent with diffusion-limited Wilson-Frenkel kinetics rather than the collision-limited regime. Based on multiple statistically independent simulations, a time-temperature-transformation (TTT) diagram for crystallisation onset is constructed. The TTT curve exhibits a nose near $0.5 T_{\mathrm{m}}$ and $100~\mathrm{ps}$, corresponding to a critical cooling rate for vitrification on the order of $10^{13}~\mathrm{K s^{-1}}.$ The simulations reproduce the crystallisation onset time and temperature observed in time-resolved X-ray diffraction experiments on optically molten Pd thin films quenched at $5 \times 10^{11}~\mathrm{K s^{-1}}.$ These results indicate that homogeneous, rather than heterogeneous, nucleation governs the achievable supercooling in the experimentally studied films.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。