PolyJarvis:用于自主聚合物分子动力学模拟的LLM代理

PolyJarvis: An LLM-Orchestrated Agent for Automated All-Atom Molecular Dynamics of Amorphous Homopolymers

Carnegie Mellon University(卡内基梅隆大学)

Alexander Zhao, Achuth Chandrasekhar, Amir Barati Farimani

AI总结:

PolyJarvis结合大语言模型与RadonPy平台,通过MCP服务器实现从自然语言输入自主执行聚合物分子动力学模拟,预测密度、体积模量和玻璃化温度等性质,验证结果在不同聚合物中表现良好。

摘要:

所有原子分子动力学(MD)模拟可以基于分子结构预测聚合物性质,但其执行需要专业知识,如力场选择、系统构建、平衡和性质提取。我们提出了PolyJarvis,一种结合大语言模型(LLM)与RadonPy模拟平台的代理,通过Model Context Protocol(MCP)服务器实现从自然语言输入到聚合物性质预测的端到端流程。给定聚合物名称或SMILES字符串,PolyJarvis可自主执行单体构建、电荷分配、聚合、力场参数化、GPU加速平衡和性质计算。验证在聚乙烯(PE)、无序聚苯乙烯(aPS)、聚甲基丙烯酸甲酯(PMMA)和聚乙二醇(PEG)上进行。结果表明,对于aPS和PMMA,密度预测误差在0.1-4.8%之间,体积模量误差在17-24%之间。PMMA的玻璃化温度(Tg)(395 K)与实验值匹配在+10-18 K内,而其余三种聚合物的Tg高估在+38至+47 K(相对于上限实验值)。8个性质-聚合物组合中有5个满足严格接受标准。对于缺乏合适无定形相实验参考的案例,报告与先前MD文献的一致性。剩余Tg失败主要归因于MD冷却速率偏置,而非代理误差。本工作证明了LLM驱动的代理能够自主执行聚合物MD工作流程,产生与专家运行模拟一致的结果。

英文摘要:

All-atom molecular dynamics (MD) simulations can predict polymer properties from molecular structure, yet their execution requires specialized expertise in force field selection, system construction, equilibration, and property extraction. We present PolyJarvis, a platform in which a planning agent produces a validated run plan that deterministic stage scripts execute through established simulation toolkits, Enhanced Monte Carlo (EMC) for system construction and LAMMPS for molecular dynamics, exposed as Model Context Protocol (MCP) servers, with a recovery agent consulted only on structured failures and within a fixed decision budget. Given a repeat-unit SMILES string and target properties, PolyJarvis constructs the amorphous cell, equilibrates it under a mechanized convergence gate, and computes target properties. Validation is conducted on seven amorphous homopolymers, each run as three replicates that share a protocol frozen per system and use independent random seeds, namely polyethylene (PE), atactic polystyrene (aPS), syndiotactic poly(vinyl chloride) (sPVC), poly(L-lactic acid) (PLLA), poly(ethylene glycol) (PEG), poly(ether ether ketone) (PEEK), and polysulfone (PSU). Against experimental references, 13 of 19 graded comparisons meet the acceptance criteria (density 5 of 7, glass transition 4 of 7, bulk modulus 4 of 5). The failures are concentrated in the PCFF systems: under-density of aPS and PEG, overestimated glass transitions of the stiff PLLA and PEEK backbones, and an overstiff PEG bulk modulus.