消除阳极氧化Ni-Ti-O纳米孔阵列中不规则表面层
Eliminating the irregular surface layer of anodically-grown Ni-Ti-O nanopore arrays in a two-stage anodization
AI总结:
通过两阶段阳极氧化工艺,去除Ni-Ti-O纳米孔阵列的不规则表面层,实现高规则性和厚层厚度,以提高表面积性能。
摘要:
通过阳极氧化生长的纳米孔(NPs)部分被相对较致密的表面氧化层所掩盖,这限制了这些纳米结构的体积表面积。在本研究中,使用含有乙二醇、水和氯化钠的电解液,在静态和搅拌的电解液阶段对硝合金(NiTi)进行阳极氧化,旨在去除不规则的表面阵列同时获得厚的纳米孔层。电子显微照片显示,静态电解液中的阳极氧化提供了由不规则表面层覆盖的受控厚度的纳米孔层。相比之下,在搅拌电解液中阳极氧化减少了厚度和不规则性,这些由纳米孔顶部、边缘和底部的溶解动力学差异控制。为了同时受益于氧化层的厚度和规则性,发现静态和然后搅拌电解液条件下的两阶段阳极氧化是有效的。在静态电解液中进行30分钟阳极氧化后,随后在搅拌条件下进行30分钟阳极氧化,提供了氧化阵列中最高的规则性,导致纳米孔直径约为40nm,层厚度约为11μm。在静态然后搅拌电解液条件下进行两阶段阳极氧化,旨在促进纳米孔结构以满足对更高表面积应用的需求。
英文摘要:
Nanopores (NPs) grown by anodizing can be partially hidden beneath a relatively compact surface oxide layer, which limits the volumetric surface area of these nanostructures. In this work, nitinol (NiTi) alloy was anodized in an electrolyte containing ethylene glycol, water, and sodium chloride in static and stirred electrolyte stages with the aim of removing the irregular surface array while achieving a thick NP layer. Electron micrographs showed that anodization in the static electrolyte provides a controlled thickness of NP layers covered by an irregular surface layer. In contrast, anodizing in the stirred electrolyte reduced the thickness and the degree of irregularity, which were controlled by the different kinetics of dissolution at the tops, perimeters and bottoms of NPs. To benefit simultaneously from the thickness and regularity of the oxide layers, two-stage anodizing under static and then stirred electrolyte conditions was found to be effective. Following a 30 min anodization in the static electrolyte, anodizing for 30 min under the stirred conditions provided the highest regularity in the oxide array, resulting in NPs of almost 40 nm and 11 μm in diameter and layer thickness, respectively. Two-stage anodizing under static then stirred electrolyte conditions is proposed in order to promote NP structures for applications demanding higher surface areas.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。