基于纤维素-聚丙烯酰胺复合水凝胶的有前景软骨植入物特性:为期90-120天的体内试验结果
Properties of promising cartilage implants based on cellulose-polyacrylamide composite hydrogels: results of in vivo tests carried out over a period of 90-120 days
AI总结:
本文研究了纤维素-聚丙烯酰胺复合水凝胶作为软骨植入物在兔子膝关节内90-120天的表现,证实其力学性能稳定且接近天然软骨,并发现离子型植入物可抑制矿化。
摘要:
高强度纤维素-聚丙烯酰胺复合水凝胶通过在预先形成的再生植物纤维素物理网络内部进行丙烯酰胺的自由基聚合合成。对这些水凝胶的酰胺基团进行部分水解,得到水解度分别为0.1和0.25的离子型形式。将三种组成的圆柱形水凝胶样品植入兔子股骨膝关节预先形成的骨软骨缺损中。在植入后长达90天和120天的体内试验过程中,未发现受试植入物有任何迁移或崩解迹象。详细研究了原始水凝胶植入物以及体内实验后从关节中取出的植入物的力学行为。通过SEM结合EDX方法研究了取出植入物的形貌和化学组成。所得结果表明,水凝胶植入物的力学特性在体内试验后实际上保持不变。取出的植入物以及初始水凝胶均能承受振幅高达50%的循环压缩载荷。在这些试验中记录到高达3-10 MPa的压缩应力,这与多位作者在相同载荷条件下对天然关节软骨所获得的数据接近。揭示了非离子型和离子型植入物邻近软骨下骨区域在化学组成和形貌上的主要差异。若非离子型植入物在该区域观察到聚合物水凝胶网络内部形成磷酸钙的强烈矿化现象,则离子型植入物的边界区域实际上不发生矿化。
英文摘要:
High-strength composite hydrogels cellulose-polyacrylamide were synthesized by free-radical polymerization of acrylamide conducted inside the previously formed physical network of regenerated plant cellulose. Partial hydrolysis of the amide groups of these hydrogels yielded their ionic forms with a degree of hydrolysis of 0.1 and 0.25. The cylindrical hydrogel samples of three compositions were implanted in the preformed osteochondral defects of the rabbit's femoral knee joints. No signs of migration or disintegration of the tested implants were revealed in the course of in vivo tests as long as 90 and 120 days after the implantation. The mechanical behavior of both the virgin hydrogels-implants and the implants extracted from the joints after in vivo experiments was studied in detail. The morphology and chemical composition of the extracted implants were studied by SEM combined with the EDX method. The results obtained were shown that the mechanical characteristics of hydrogel implants remained practically unchanged after in vivo tests. The extracted implants, as well as the initial hydrogels, endured cyclic compression loading at the amplitude up to 50 %. Compression stresses up to 3-10 MPa were recorded in these tests, which is close to the data obtained by several authors for natural articular cartilages in the same conditions of loading. The principal differences in the chemical composition and morphology of the implant area adjacent to the subchondral bone for non-ionic and ionic types of implants have been revealed. If for non-ionic types of implants in this area intensive mineralization with formation of calcium phosphates inside the polymeric hydrogel network is observed, the border area of ionic implants practically does not undergo mineralization.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。