LBNF吸收堆芯块关键铝焊缝焊接工艺优化
Optimization of a Welding Procedure for Making Critical Aluminum Welds on the LBNF Absorber Core Block
AI总结:
针对LBNF铝制吸收堆芯块的焊接需求,通过调整钨极参数和预热工艺优化钨极气体保护焊规范,有效减少焊缝钨夹杂物,所有试样均通过ASME B31.3检验。
摘要:
LBNF吸收器由13块6061-T6铝制堆芯块组成。堆芯块采用去离子(DI)水冷却,该冷却水在束流运行期间会产生放射性。冷却水流经堆芯块内的深孔钻削通道。为在铝制堆芯块上制备符合美国国家航空标准1514 I类质量的焊缝,研究人员开展了焊接质量优化工作,但并非所有情况都能成功。研究对现有钨极气体保护焊工艺规范进行了微调,以在大多数情况下减少并消除焊缝中可检测到的钨夹杂物。不过,所有焊接试样均通过了管道规范ASME B31.3常规流体工况的焊接检验。研究对钨电极的直径、类型和生产厂家进行了变量控制,部分试样进行了预热,其余则未预热。观察发现,采用直径为5/32英寸的大直径电极并对接头进行预热时,焊缝中的钨夹杂物数量最少。研究假设,较细的电极容易损耗,在焊接过程中会脱落并滞留在熔池中;未预热试样与热电极之间的较大温差会进一步加剧这种损耗。
英文摘要:
The LBNF Absorber consists of thirteen 6061-T6 aluminum core blocks. The core blocks are water cooled with de-ionized (DI) water which becomes radioactive during beam operations. The cooling water flows through gun-drilled channels in the core blocks. A weld quality optimization was performed to produce National Aeronautical Standard 1514 Class I quality welds on the aluminum core blocks. This was not successful in all cases. An existing Gas Tungsten Arc Welding Procedure Specification was fine tuned to minimize, in most cases, and eliminate detect-able tungsten inclusions in the welds. All the weld coupons, however passed welding inspection as per the piping code: ASME B31.3 Normal Fluid Service. Tungsten electrode diameter, type, and manufacturer were varied. Some of the samples were pre-heated and others were not. It was observed that larger diameter electrodes, 5/32 in., with pre-heated joints resulted in welds with the least number of tungsten inclusions. It is hypothesized that thinner electrodes breakdown easily and get lodged into the weld pool during the welding process. This breakdown is further enhanced by the large temperature differential between the un-preheated sample and the hot electrode.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。