arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2406.01165cond-mat.mtrl-sciphysics.app-ph
收藏

评估热塑性聚合物在低温密封应用中的潜力:应变率与温度的影响

Evaluating the potential of thermoplastic polymers for cryogenic sealing applications: strain rate and temperature effects

Zhenzhou Wang, Wendell Bailey, Junyao Song, Lingfeng Huang, Yifeng Yang

AI总结:

本文研究了PTFE、PEEK和UHMWPE在室温和低温(77 K、20 K)及不同应变率下的拉伸性能、热膨胀系数与失效机制,发现PEEK在20 K下收缩最小,为低温燃料系统密封材料选择提供了依据。

摘要:

液氢和液化天然气等低温燃料作为多功能且可持续的能源载体,正在彻底改变航空航天、汽车、船舶和发电等多个行业。在低温燃料系统中,热塑性聚合物可以作为金属密封件的合适替代品。然而,目前关于热塑性塑料在低温下行为的研究有限,特别是在20开尔文(K)的液氢温度下。本文测量了三种常用热塑性塑料:PTFE、PEEK和UHMWPE在室温(RT)、77 K和20 K以及四种应变率下的拉伸性能和热膨胀系数。此外,还进行了进一步的显微分析,以了解将降低的温度与不同的应变率相结合时发生的失效机制。每种聚合物的拉伸强度从RT到77 K有所增加,而从77 K到20 K则有所下降。当温度从RT降至20 K时,弹性模量趋于增加,而在失效时记录的应变减小。通过对PEEK和UHMWPE的显微观察,温度从77 K降至20 K导致了更大的瞬时断裂,断裂面呈多面状,在断裂区内包含许多小的镜面状以及不透明或雾状子区域。对于PTFE,表面形貌表现出对低温下应变率增加的不敏感,显微观察显示,当温度从77 K降至20 K时,断裂界面内发现的韧窝尺寸变得更小。最后,发现PEEK在20 K下的收缩量远小于PTFE和UHMWPE,这与其在三种聚合物中具有最高的玻璃化转变温度相符,这通常是在试图识别在低温下倾向于表现出较小收缩的聚合物时的一个良好指标。

英文摘要:

Cryogenic fuels, such as liquid hydrogen and liquid natural gas, emerge as versatile and sustainable energy carriers that are revolutionising various industries including aerospace, automotive, marine, and power generation. Thermoplastic polymers can be a suitable alternative to metal seals in cryogenic fuel systems. However, there is limited study about the behaviours of thermoplastics at cryogenic temperatures, especially at liquid hydrogen temperature of 20 Kelvin (K). This paper measured the tensile properties and coefficient of thermal expansion of three popular thermoplastics: PTFE, PEEK and UHMWPE at room temperature (RT), 77 K and 20 K and at four strain rates. Further microscopic analysis was also conducted to understand the failure mechanisms occurring when combining reduced temperature with varying strain rate. The tensile strength of each polymer increased from RT to 77 K and decreased from 77 K to 20 K. Elastic modulus tended to increase, and the strain recorded at failure decreased when reducing temperature from RT to 20 K. From microscopic observation of PEEK and UHMWPE, a reduction in temperature from 77 K to 20 K resulted in a larger instantaneous fracture, with multi-faceted fracture surfaces containing many small mirror like and opaque or misty sub-regions within the fracture zone. For PTFE, the surface morphology exhibited an insensitivity to the increase in strain rate at cryogenic temperatures, and the microscopy showed how the size of dimples found within the fracture interface became smaller when temperature was reduced from 77 K to 20 K. Finally, PEEK was found to contract much less than PTFE and UHMWPE at 20 K, in agreement to it having the highest glass transition temperature of the three polymers, which is normally a good indicator when attempting to identify polymers that will tend to exhibit smaller contraction at cryogenic temperatures.