采用光电联合监测方法追踪 R-HiPIMS TiO$_2$ 沉积过程漂移
Using a coupled optical and electrical monitoring method to follow the R-HiPIMS TiO$_2$ deposition process drifts
AI总结:
本文通过光学与电学联合测量,研究 R-HiPIMS TiO$_2$ 沉积中靶材侵蚀和基片架温度导致的过程漂移,证明该方法能灵敏识别沉积速率、发射强度及氧原子变化。
摘要:
本工作采用光学与电学放电联合测量手段,研究在固定占空比2%、重复频率1 kHz下运行的反应式 HiPIMS TiO$_2$ 沉积过程的等离子体状态。研究重点考察在固定工作压力的 Ar/O$_2$ 混合气体中,靶材侵蚀和基片架温度两方面的影响。首先,随着跑道形状随靶材使用而演变,沉积速率发生变化,所测发射强度也以相同方式变化。其次,在纯 Ar 中将加热器设定为400 $^\circ$C时,涂层显得更薄,且光发射光谱测量显示存在氧原子。因此,光电联合测量结果具有足够灵敏度,可追踪该过程的潜在漂移。
英文摘要:
In this work, coupled optical and electrical discharge measurements have been implemented to investigate the plasma state of a reactive HiPIMS TiO$_2$ deposition process running at a fixed duty cycle of 2% and at a repetition rate of 1 kHz. Investigations focus on both the effect of the erosion target and substrate-holder temperature in an Ar/O$_2$ gas mixture at fixed working pressure. First, as the racetrack shape evolves with the use of the target, the deposition rate is modified, in the same way as the emission intensity measured. Second, with the heater set at 400 $^\circ$C in pure Ar, the coating appears thinner, and the optical emission spectroscopy measurement reveals the presence of oxygen atoms. Thus, the results from the coupled optical and electrical measurements are sensitive enough to track potential drift of the process.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。