增材制造316L不锈钢的氢脆敏感性:后处理、打印方向、温度与预应变的影响
Hydrogen embrittlement susceptibility of additively manufactured 316L stainless steel: influence of post-processing, printing direction, temperature and pre-straining
AI总结:
本文研究了增材制造316L不锈钢在不同后处理、打印方向、温度和预应变条件下的氢脆行为,发现热等静压态AM 316L在低温充氢后延展性可达传统制造材料近两倍,其优异性能源于应变诱导马氏体形成倾向的降低。
摘要:
通过单轴拉伸实验,在室温和-50°C下评估了后处理对采用激光粉末床熔融技术制备的增材制造(AM)316L不锈钢氢脆行为的影响。在室温无氢条件下,所有四种评估的AM状态(打印态(AB)、退火态(ANN)、热等静压态(HIP)以及热等静压加30%冷加工态(CW))相对于传统制造(CM)316L不锈钢均表现出显著降低的延展性。AM材料在有无氢条件下均表现出对打印方向的敏感性,X方向的屈服强度显著提高,Z方向的延展性增强。相反,在-50°C下对未充氢试样的测试表明,CM、AB、ANN和HIP状态之间的延展性相似。充氢后,在室温下所有四种AM状态的延展性与CM 316L相似,其中HIP状态实际上超过了CM材料。关键的是,在-50°C下对充氢试样的测试表明,HIP AM 316L状态的延展性几乎是CM 316L的两倍。这种改进的性能即使在冷加工后仍然保持,因为CW AM 316L在-50°C充氢后表现出与CM 316L相当的延展性,尽管其屈服强度高出2倍。铁素体仪测量表明,这种性能提升与AM 316L在变形过程中形成应变诱导马氏体的倾向降低有关,即使在经过显著的后处理之后也是如此。这些结果表明,AM 316L可以采用典型工艺进行后处理,从而表现出与CM 316L相似甚至更好的抗氢脆性能。
英文摘要:
The influence of post-build processing on the hydrogen embrittlement behavior of additively manufactured (AM) 316L stainless steel fabricated using laser powder bed fusion was assessed at both room temperature and -50$^\circ$ C via uniaxial tensile experiments. In the absence of hydrogen at ambient temperature, all four evaluated AM conditions (as-built (AB), annealed (ANN), hot isostatic pressed (HIP), and HIP plus cold worked (CW) to 30\%) exhibit notably reduced ductility relative to conventionally manufactured (CM) 316L stainless steel. The AM material exhibits sensitivity to the build direction, both in the presence and absence of hydrogen, with a notable increase in yield strength in the X direction and enhanced ductility in the Z direction. Conversely, testing of non-charged specimens at -50$^\circ$ C revealed similar ductility between the CM, AB, ANN, and HIP conditions. Upon hydrogen charging, the ductility of all four AM conditions was found to be similar to that of CM 316L at ambient temperature, with the HIP condition actually exceeding the CM material. Critically, testing of hydrogen-charged samples at -50$^\circ$ C revealed that the ductility of the HIP AM 316L condition was nearly double that observed in the CM 316L. This improved performance persisted even after cold working, as the CW AM 316L exhibited comparable ductility to CM 316L at -50 C after hydrogen charging, despite having a 2-fold higher yield strength. Feritscope measurements suggest this increased performance is related to the reduced propensity for AM 316L to form strain-induced martensite during deformation, even after significant post-processing treatments. These results demonstrate that AM 316L can be post-processed using typical procedures to exhibit similar to or even improved resistance to hydrogen embrittlement relative to CM 316L.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。