arXiv 2403.19544cond-mat.softcond-mat.mtrl-sci
收藏

树脂分子量对涂层干燥动力学与流挂的影响

Impact of Resin Molecular Weight on Drying Kinetics and Sag of Coatings

Marola W. Issa, Steve V. Barancyk, Reza M. Rock, James F. Gilchrist, Christopher L. Wirth

AI总结:

本文研究树脂分子量与溶剂对涂层干燥和流挂的影响,发现高分子量树脂虽延长干燥时间,但因显著提高粘度而有效抑制流挂。

摘要:

本文研究了树脂分子量和溶剂选择对聚合物薄膜干燥动力学及流挂速度的影响。这些薄膜厚度约为60微米至120微米,由45%重量分数的聚合物树脂配制而成,所用溶剂为两种具有不同相对蒸发速率(RER)的溶剂体系。首先采用重量分析法跟踪干燥动力学,并利用一维扩散模型计算表观溶剂扩散系数。此外,通过光学轮廓术跟踪薄膜厚度。测量结果表明,在固定分子量条件下,高RER溶剂的干燥动力学约提高两倍,而表观扩散系数随聚合物分子量增加而趋于增大。在相同的刮涂刀间隙下,由较高分子量树脂配制的薄膜具有更高的初始粘度和厚度。由此推断,较高分子量下较高的表观扩散系数可归因于较厚薄膜蒸发时间延长的效应。使用可变角度检测显微镜(VAIM)在5度倾角下测量了这些体系沿薄膜厚度方向的流挂速度。测量结果显示,较薄且粘度较低的薄膜流挂速度增大,这一结果有些出乎意料,因为与较厚薄膜相比,较薄薄膜所承受的重力应力更低且干燥时间更短。基于这些数据我们得出结论:采用较高分子量树脂配制涂层虽然可能延长干燥时间,但由于粘度对这些现象的巨大影响,往往能够抑制流挂。

英文摘要:

The work herein investigates the impact of resin molecular weight and solvent choice on drying kinetics and sag velocity in polymer films. These films, ranging in thickness from ~60 micrometer to ~120 micrometer were formulated with 45% by weight polymer resin in one of two solvent packages with different relative evaporation rates (RER). Gravimetry was initially used to track drying kinetics and a one-dimensional diffusion model was utilized to compute the apparent solvent diffusivity. In addition, the film thickness was tracked with optical profilometry. Results from these measurements showed that for fixed molecular weight the drying kinetics increased by approximately two-fold for the high RER solvent, whereas the apparent diffusivity tended to increase with increasing polymer molecular weight. Films formulated from higher molecular weight resins had greater initial viscosities and thicknesses for identical draw down blade clearance. By extension, the higher apparent diffusivities at greater molecular weights were attributed to effects of prolonged evaporation times for the thicker films. The sag velocity was measured through the thickness of the film for these systems at a 5 degree incline using the Variable Angle Inspection Microscope (VAIM). Measurements showed an increase in sag velocity for thinner and less viscous films, which was somewhat surprising both because a thinner film will experience lower gravitational stress and quicker drying times as compared to a thicker film. From these data we conclude that formulating a coating with higher molecular weight resin, although likely to increase drying time, will tend to deter sag because of the large impact of viscosity on these phenomena.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑